MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Thermal Ceramics K-Shield LS Felt
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: K-Shield Felt products are produced from premium, cleaned Kaowool high-purity fibers and a special thermosetting binder system in a unique paper-making process. The cleaning process improves the thermal conductivity, insulating value, and vibration resistance of the felt, while also making it an ideal product for die-cutting, fabrication, and handling. K-Shield Felts are both compressible and resilient, while exhibiting excellent flexibility and handling strengths. The special binder system eliminates smoke problems and allows for minimal off-gassing. Due to their unique semi-rigid yet flexible form, K-Shield Felts offer some special properties in comparison to traditional blankets and papers.

The standard K-Shield Felt, K-Shield Felt LS, and K-Shield Felt AG are premium, low-shot products produced from cleaned high-purity ceramic fibers. The K-Shield Felt LS is a very clean, lower-shot product developed for those very demanding applications. These products have very low thermal conductivities and exhibit excellent vibration resistance.

The K-Shield Felt AG is designed specifically for aerospace insulation applications and is approved for both the BMS9-19 and AMS 3680-Rev. C specifications. These approvals include meeting specific tests related to optimum performance in aerospace insulation applications.

Features:

  • Low thermal conductivity and heat storage
  • Excellent flexibility with good handling strength for fabrication and die-cutting
  • High temperature stability
  • Low organic binder content with minimal off-gassing
  • Low shot (unfiberized material) content
  • Lightweight, yet resilient
  • Continuous use limit of 2300°F (1260°C)
  • Applications:

  • Automotive heat shields and muffler insulation
  • Aerospace insulation
  • High-temperature gasketing
  • Commercial and domestic appliance insulation
  • Expansion joints
  • Parting agent in heat treating and metal working
  • Glassware separator
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.0960 g/cc0.00347 lb/in³
    Loss On Ignition 2.0 - 5.0 %2.0 - 5.0 %
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength, Ultimate 0.0345 MPa5.00 psiFired
     0.0689 - 0.138 MPa10.0 - 20.0 psi
     
    Thermal PropertiesMetricEnglishComments
    Thermal Conductivity  0.0548 W/m-K
    @Temperature 260 °C
    0.380 BTU-in/hr-ft²-°F
    @Temperature 500 °F
     0.0865 W/m-K
    @Temperature 538 °C
    0.600 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
     0.133 W/m-K
    @Temperature 816 °C
    0.920 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
     0.197 W/m-K
    @Temperature 1090 °C
    1.37 BTU-in/hr-ft²-°F
    @Temperature 2000 °F
    Melting Point 1760 °C3200 °F
    Maximum Service Temperature, Air 1260 °C2300 °F
     
    Component Elements PropertiesMetricEnglishComments
    Al2O3 51 %51 %
    SiO2 49 %49 %
     
    Descriptive Properties
    Other Element Contenttraces

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Zircar Refractory Composites RS-3000 ALUMINA FELT
    Morgan Advanced Ceramics Kaowool HP Veneering Module Thermal Ceramic
    Morgan Advanced Ceramics Kaowool Ceramic Felt 1260 Thermal Ceramic
    Morgan Advanced Ceramics Kaowool C Veneering Module Thermal Ceramic
    Morgan Advanced Ceramics Green Glass Paper Thermal Ceramic

    CTHERM247 / 2567

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.