MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Nucrel® 2806 Ethylene-Acrylic Acid Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Acrylic Acid

Material Notes: Nucrel® 2806 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for exterior applications and painted or plated for special decorative effects.

Typical Applications:

  • Heat sealable coating
  • Base resin for color concentrates
  • Metal coating
  • Dispersions
  • Paper coating
  • Nonwoven binding

Features:

  • Good adhesion to metal, glass, cellulosic and other polar substrates
  • May be processed into aqueous amines and alkali based dispersions

Information provided by DuPont.

This product line/trade name was acquired by Dow, but this specific grade was discontinued prior to the acquisition.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.944 g/cc0.0341 lb/in³ASTM D792
Melt Index of Compound 60 g/10 min
@Load 2.16 kg,
Temperature 190 °C
60 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4242Initial (peak) hardness; ASTM D2240
Tensile Strength at Break 22.6 MPa3280 psiType IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638
Elongation at Break 464 %464 %Type IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638
Flexural Modulus 0.0386 GPa5.60 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Tensile Impact Strength  25.0 kJ/m²
@Temperature -40.0 °C
11.9 ft-lb/in²
@Temperature -40.0 °F
ASTM D1822S
 372 kJ/m²
@Temperature 23.0 °C
177 ft-lb/in²
@Temperature 73.4 °F
ASTM D1822S
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 48.0 °C118 °FRate B; ASTM D1525
 
Processing PropertiesMetricEnglishComments
Zone 1 160 °C320 °F
Zone 2 182 °C360 °F
Zone 3 193 °C379 °F
Zone 4 204 °C399 °F
Zone 5 204 °C399 °F
Die Temperature 204 °C400 °F
Melt Temperature 149 - 232 °C300 - 450 °F
 
Descriptive Properties
Acrylic Acid Content18 wt.%DuPont Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin
Arkema LOTADER® 8200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
Dow Bynel® 2022 Acid-Modified Ethylene Terpolymer Adhesive Resin
Dow Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
Dow Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating

PDUPM109 / 33776

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.