MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient LubriOne™ NN-30GF/10T WHT Polyamide 66 (Nylon 66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Water Absorption 0.50 %
@Temperature 23.0 °C
0.50 %
@Temperature 73.4 °F
@ 24 hrs; Internal Method
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D  82
@Temperature 23.0 °C
82
@Temperature 73.4 °F
15 sec; ASTM D2240
 83
@Temperature 23.0 °C
83
@Temperature 73.4 °F
ASTM D2240
Tensile Strength 172 MPa24900 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 9.65 GPa1400 ksiASTM D638
Flexural Strength 241 MPa35000 psiASTM D790
Flexural Modulus 9.65 GPa1400 ksiASTM D790
Izod Impact, Notched 1.10 J/cm2.06 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 8.50 kV/mm
@Temperature 23.0 °C
216 kV/in
@Temperature 73.4 °F
Method A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 244 °C471 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 288 - 299 °C550 - 570 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 71.1 - 82.2 °C160 - 180 °F
 
Descriptive Properties
AdditiveLubricant
AppearanceWhite
FeaturesLubricated
FormsPellets
Generic MaterialNylon 66
Generic NamePolyamide 66 (Nylon 66)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAppliance Components
 Automotive Applications
 Bearings
 Business Equipment
 Consumer Applications
 Conveyor Parts
 Gears
 Industrial Applications
 Printer Parts
 Pulleys
 Rollers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient LubriOne™ NN-000/20T Polyamide 66 (Nylon 66)
Sax Polymers SAXAMID 226F6T3 Nylon 6.6, 30% Glass Fiber
Kuraray Genestar™ G1301A-M61 Nylon, 30% Glass Filled
Avient LubriOne™ NN-30GF/13T-2S Black Polyamide 66 (Nylon 66)
Avient LubriOne™ NN-30CF/15T-02S black Polyamide 66 (Nylon 66)

PH0POL1104 / 145673

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.