MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals Sclair® IG454-A Injection Molded HDPE Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: IG454-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. IG454-A is subject to the specific limitation that it may contact food only at temperatures of 212°F and below.

NOVA Chemicals' polyethylene resins are chemically and biologically inert.

Features: Superior stiffness allows for part thinwalling and enhanced stacking strength, Lower viscosity for exceptional processability yielding shorter cycle times and energy savings, Exceptional solid state properties provide improved impact resistance and ESCR, Good organoleptic properties and natural colorAdditives: Antioxidant

Applications: Shipping pails (both food and industrial), Storage bins and totes, Caps and closures, Crates

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 16.0 MPa2320 psi50 mm/min test speed; ASTM D 638
Tensile Strength, Yield 22.3 MPa3230 psi50 mm/min test speed; ASTM D 638
Elongation at Break 650 %650 %50 mm/min test speed; ASTM D 638
Elongation at Yield 9.0 %9.0 %50 mm/min test speed; ASTM D 638
Flexural Modulus, 1% Secant 960 MPa139000 psiASTM D 790

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NOVA Chemicals Sclair® IG464-C Injection Molded HDPE Resin
Dow DOWLEX™ IP-60 High Density Polyethylene
ExxonMobil HD 56200 High Density Polyethylene Resin
Total 6280 High Density Polyethylene, Injection Molding Resin
Braskem JV060U Injection Molding High Density Polyethylene

PNOV872 / 108479

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.