MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay CYCOM® 2020 Epoxy + T800-6K 2X2T Twill 200 Prepreg with Post-Cure
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: CYCOM® 2020 is a versatile curing, toughened epoxy resin that can be cured from 180°F to 350°F (80°C to 180°C), depending on service temperature requirements. This prepreg resin extracts the maximum possible performance from carbon fibers. The excellent overall balance of properties delivered by CYCOM 2020 has made it the product of choice for many Formula 1 race teams in structural applications. CYCOM 2020 can be either autoclave or vacuum bag cured. Free-standing postcures can also be employed. A one hour cure at 275°F (135°C) gives a Tg of more than 310°F (155°C). The same cure cycle provides excellent mechanical properties with retention of those properties at temperature; 70% of shear strength is retained at 250°F (120°C). CYCOM 2020 is available on both woven and unidirectional carbon, glass and aramid fiber and has a tack-life under ambient conditions in excess of four weeks, maintaining good drape and tack characteristics throughout.

Features & Benefits:

  • Excellent translation of fiber properties
  • Excellent retention of mechanical properties at 240°F (120°C) temperature
  • High impact resistance
  • Controlled flow
  • Good drape and tack
  • Excellent cured surface finish
  • Shop life of 8 weeks at ambient temperature, 75°F (24°C)
Suggested Applications:
  • High stress extreme performance mast and boom applications
  • Structural Formula 1 applications
Property data for CYCOM 2020 T800-6K 2X2T Twill 200 42% Resin Content with Standard Cure (1 hour at 275°F (135°C)) plus post-cure (2 hours at 356°F (180°C)).

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³Cured Resin
Viscosity  2000 cP
@Temperature 120 °C
2000 cP
@Temperature 248 °F
Neat Resin
 5000 cP
@Temperature 132 °C
5000 cP
@Temperature 270 °F
Neat Resin
 10000 cP
@Temperature 94.0 °C
10000 cP
@Temperature 201 °F
Neat Resin
 100000 cP
@Temperature 63.0 °C
100000 cP
@Temperature 145 °F
Neat Resin
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 883 MPa
@Temperature 177 °C
128000 psi
@Temperature 351 °F
0° Orientation; ASTM D3039
Tensile Modulus 78.0 GPa
@Temperature 177 °C
11300 ksi
@Temperature 351 °F
0° Orientation; ASTM D3039
Flexural Strength 462 MPa
@Temperature 177 °C
67000 psi
@Temperature 351 °F
0° Orientation; ASTM D790
Flexural Modulus 53.0 GPa
@Temperature 177 °C
7690 ksi
@Temperature 351 °F
0° Orientation; ASTM D790
Compressive Strength 373 MPa
@Temperature 177 °C
54100 psi
@Temperature 351 °F
0° Orientation; ASTM D695
Compressive Modulus 77.0 GPa
@Temperature 177 °C
11200 ksi
@Temperature 351 °F
0° Orientation; ASTM D695
Shear Modulus 1.00 GPa
@Temperature 177 °C
145 ksi
@Temperature 351 °F
±45° Orientation, In-plane; ASTM D3518
Shear Strength  40.0 MPa
@Temperature 177 °C
5800 psi
@Temperature 351 °F
Interlaminar Short Beam; ASTM D2344
 57.9 MPa
@Temperature 177 °C
8400 psi
@Temperature 351 °F
±45° Orientation, In-plane; ASTM D3518
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 116 °C240 °FExcellent Mechanical Property Retention
Glass Transition Temp, Tg 100 °C212 °FCure Cycle: 10 hour at 176°F (80°C)
 120 °C248 °FPeak tan d, Cure Cycle: 10 hour at 176°F (80°C)
 126 °C259 °FCure Cycle: 4 hours at 212°F (100°C)
 150 °C302 °FPeak tan d, Cure Cycle: 4 hours at 212°F (100°C)
 151 °C304 °FCure Cycle: 0.5 hour at 275°F (135°C)
 153 °C307 °FCure Cycle: 1 hour at 275°F (135°C)
 170 °C338 °FCure Cycle: 1 hour at 302°F (150°C)
 177 °C351 °FPeak tan d, Cure Cycle: 0.5 hour at 275°F (135°C)
 177 °C351 °FPeak tan d, Cure Cycle: 1 hour at 275°F (135°C)
 185 °C365 °FCure Cycle: 1 hour at 275°F (135°C) plus 2 hours at 356°F (180°C)
 190 °C374 °FPeak tan d, Cure Cycle: 1 hour at 302°F (150°C)
 205 °C401 °FPeak tan d, Cure Cycle: 1 hour at 275°F (135°C) plus 2 hours at 356°F (180°C)
 
Processing PropertiesMetricEnglishComments
Processing Temperature 82.2 - 177 °C180 - 350 °FCure Temp. Range
 135 °C
@Time 3600 sec
275 °F
@Time 1.00 hour
Standard Cure Cycle
Gel Time 15.0 min
@Temperature 120 °C
15.0 min
@Temperature 248 °F
Shelf Life 12.0 Month
@Temperature <=-12.0 °C
12.0 Month
@Temperature <=10.4 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay CYCOM® 2020 Epoxy + T800-6K 2X2T Twill 200 Prepreg, without Post-Cure
Solvay CYCOM® 5320-1 Epoxy with T40/800B Unidirectional Tape Composite
Solvay CYCOM® 985 Epoxy + Carbon Fabric Laminate
Solvay CYCOM® 985 Epoxy + Carbon Uni-Tape Laminate
Solvay CYCOM® E773FR Epoxy + Plain Weave Fabric Prepreg

PCYTED131e / 193486

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.