MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HTA 001HD High Density Polyethylene (HMW) Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: HTA 001HD is a high weight HDPE film grade. Films made from HTA 001HD exhibit excellent impact and toughness properties as well as high stiffness.

Availability: Africa & Middle East and Asia Pacific

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Blown Film
  • Grocery Sacks
  • Liners
  • Produce Bags
  • Produce Bags on a Roll
  • Refuse Bags
  • Thin Gauged Consumer Bags
  • Trash Can Liners

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.952 g/cc0.0344 lb/in³ASTM D4883
Melt Flow 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 40.7 MPa5900 psiASTM D882
Film Tensile Strength at Yield, TD 30.3 MPa4400 psiASTM D882
Film Elongation at Break, MD 220 %220 %ASTM D882
Film Elongation at Break, TD 430 %430 %ASTM D882
Elmendorf Tear Strength MD 8.0 g8.0 gASTM D1922
Elmendorf Tear Strength TD 30 g30 gASTM D1922
Dart Drop Test 190 g0.419 lbASTM D1709A
Film Tensile Strength at Break, MD 59.3 MPa8600 psiASTM D882
Film Tensile Strength at Break, TD 55.8 MPa8100 psiASTM D882
1% Secant Modulus, MD 1170 MPa170000 psiASTM D882
1% Secant Modulus, TD 1170 MPa170000 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 126 °C259 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil HTA 001HP2 High Density Polyethylene (HMW) Resin
ExxonMobil HD 6040.UV High Density Polyethylene Resin
ExxonMobil HD 7960.13 HMW Blown Film Resin
ExxonMobil HPA 020 Molding High Density Polyethylene (HMW) Resin
Equate EMDA-6147 HDPE Blow Molding Resin

PEX99322 / 175558

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.