MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Elix Polymers Elix™ 158 I ABS Polymer Modifier
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; ABS Polymer

Material Notes: High rubber content ABS modifier used to improve toughness of engineering thermoplastics and PVC.

Information provided by Elix Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.250 - 0.390 g/cc0.00903 - 0.0141 lb/in³lab (internal)
 
Processing PropertiesMetricEnglishComments
Moisture Content 1.0 - 2.0 %1.0 - 2.0 %Lab (internal)
 
Descriptive Properties
Polybutadiene Content54-58%lab internal-IR
Residual Monomers (%)max. 0.25%lab-GC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Elix Polymers Elix™ 260 G SAN Polymer Modifier
Hannam Chemical Hanalac 740 ABS, Super High Impact Grade
Global GAB-110 10% Glass Reinforced, General Purpose ABS
Covestro Bayblend® T88-2N Polycarbonate + ABS, 10% Glass Filled
Covestro Bayblend® T 88-2N Polycarbonate/ABS Blend, 10% Glass Fiber

PELIX930 / 192524

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.