MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röchling Glastic BMC 1401 GTP Glass-Reinforced Polyester  (discontinued **)
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: Data provided by Glastic Corporation.

Electrical encapsulation grade. Characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.76 g/cc0.0636 lb/in³ASTM D792
Water Absorption 0.25 %0.25 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 29.0 MPa4210 psiASTM D638
Flexural Strength 83.0 MPa12000 psiASTM D790
Compressive Strength 110 MPa16000 psiASTM D695
Izod Impact, Notched 0.800 J/cm1.50 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 11.0 kV/mm279 kV/inShort-Term, ASTM D149
Dissipation Factor 0.015
@Frequency 60 Hz
0.015
@Frequency 60 Hz
Condition A, ASTM D150; ASTM D150
Arc Resistance 190 sec190 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Röchling GLASTHERM HT220 Insulation Sheet
Röchling Glastic BMC 1403 GTP Glass-Reinforced Polyester
Röchling Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate
A. Schulman BMC 310 Cosmetic and Appliance Grade Compound
A. Schulman BMC 304 Automotive Grade Molding Compound

PGLAS0 / 41901

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.