Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber
Categories:
Polymer
;
Thermoset
;
Bismaleimide (BMI)
Material Notes:
Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2
Information provided by HexCel
Key Words:
BMI
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
112
MPa
@Temperature 177 °C
16200
psi
@Temperature 351 °F
[+/-45°]; Resin Content=27%, Fiber Volume=66%; Wet condition-96 hours in boiling H2O
138
MPa
@Temperature 177 °C
20000
psi
@Temperature 351 °F
[+/-45°]; Resin Content=27%, Fiber Volume=66%
145
MPa
@Temperature 23.0 °C
21000
psi
@Temperature 73.4 °F
[+/-45°]; Resin Content=27%, Fiber Volume=66%
2774
MPa
@Temperature 23.0 °C
402300
psi
@Temperature 73.4 °F
[0°]; Resin Content=26%, Fiber Volume=67%
Elongation at Yield
1.66 %
@Temperature 23.0 °C
1.66 %
@Temperature 73.4 °F
[0°]; Resin Content=26%, Fiber Volume=67%
Tensile Modulus
9.79
GPa
@Temperature 177 °C
1420
ksi
@Temperature 351 °F
[+/-45°]; Resin Content=27%, Fiber Volume=66%; Wet condition-96 hours in boiling H2O
15.8
GPa
@Temperature 177 °C
2290
ksi
@Temperature 351 °F
[+/-45°]; Resin Content=27%, Fiber Volume=66%
19.7
GPa
@Temperature 23.0 °C
2860
ksi
@Temperature 73.4 °F
[+/-45°]; Resin Content=27%, Fiber Volume=66%
165
GPa
@Temperature 23.0 °C
23900
ksi
@Temperature 73.4 °F
[0°]; Resin Content=26%, Fiber Volume=67%
Compressive Yield Strength
917
MPa
@Temperature 177 °C
133000
psi
@Temperature 351 °F
[0°]; Resin Content=29%, Fiber Volume=64%; Wet condition-96 hours in boiling H2O
1089
MPa
@Temperature 232 °C
157900
psi
@Temperature 450 °F
[0°]; Resin Content=29%, Fiber Volume=64%
1303
MPa
@Temperature 177 °C
189000
psi
@Temperature 351 °F
[0°]; Resin Content=29%, Fiber Volume=64%
1862
MPa
@Temperature 23.0 °C
270100
psi
@Temperature 73.4 °F
[0°]; Resin Content=29%, Fiber Volume=64%
Compressive Modulus
131
GPa
@Temperature 177 °C
19000
ksi
@Temperature 351 °F
[0°]; Resin Content=29%, Fiber Volume=64%; Wet condition-96 hours in boiling H2O
137
GPa
@Temperature 177 °C
19900
ksi
@Temperature 351 °F
[0°]; Resin Content=29%, Fiber Volume=64%
139
GPa
@Temperature 232 °C
20200
ksi
@Temperature 450 °F
[0°]; Resin Content=29%, Fiber Volume=64%
145
GPa
@Temperature 23.0 °C
21000
ksi
@Temperature 73.4 °F
[0°]; Resin Content=29%, Fiber Volume=64%
Shear Strength
27.0
MPa
@Temperature 232 °C
3920
psi
@Temperature 450 °F
Short Beam; [0°]; Resin Content=29%, Fiber Volume=64%; Wet condition-96 hours in boiling H2O
45.0
MPa
@Temperature 177 °C
6530
psi
@Temperature 351 °F
Short Beam; [0°]; Resin Content=29%, Fiber Volume=64%; Wet condition-96 hours in boiling H2O
65.0
MPa
@Temperature 232 °C
9430
psi
@Temperature 450 °F
Short Beam; [0°]; Resin Content=29%, Fiber Volume=64%
88.9
MPa
@Temperature 177 °C
12900
psi
@Temperature 351 °F
Short Beam; [0°]; Resin Content=29%, Fiber Volume=64%
118
MPa
@Temperature 23.0 °C
17100
psi
@Temperature 73.4 °F
Short Beam; [0°]; Resin Content=29%, Fiber Volume=64%
Descriptive Properties
Energy Release Rate (kJ/m2)
0.41
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber
Hexcel® HexPly® F655 Bismaleimide Resin
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber
Renegade Materials Corporation RM-3002 Bismaleimide (BMI) Resin IM7 12K Carbon Uni-tape
Quantum Composites HTC-9593 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite
PHEXC004 / 98474
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.