MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Amco PRIMATOP PP HOMO 120NA-HF Multi-Purpose Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Features:
  • medium viscosity
  • excellent processability
  • good stiffness
  • nucleation
  • anti-stat
Applications:
  • closures
  • thin wall applications
  • housewares

Former A-Top Polymers product; part of Amco product line since 2013.

Key Words: FDA 21CFR177.1520
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.907 g/cc0.0328 lb/in³ASTM D1505
Melt Index of Compound 12 g/10 min
@Temperature 230 °C
12 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 115115ASTM D785
Tensile Strength, Yield 40.0 MPa5800 psi50 mm/min; ASTM D638
Elongation at Yield 6.5 %6.5 %50 mm/min; ASTM D638
Flexural Modulus, 1% Secant 1860 MPa270000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched 0.320 J/cm
@Temperature 22.8 °C
0.600 ft-lb/in
@Temperature 73.0 °F
ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Amco PRIMATOP PP HOMO 350NA Injection Molding Polypropylene
Borealis Daploy™ WB140HMS Polypropylene
Ineos H05H-01 Polypropylene Homopolymer
Aclo Accuguard Polypropylene HP1362V2CSL Homopolymer Flame Retardant Copper Stabilized
Akro-Plastic Akromid® A3 1 L black (4652) PA 66 + PP Conditioned

PATOP022 / 79965

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.