MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Parker Chomerics CHO-THERM 1642 Thermally Conductive Silicone
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: Thermally Conductive Silicone Compound. This compound is a two-component thermally conductive adhesive/sealant/caulk/potting compound that also combines the features of silicone and ceramics. It is a two-component product that does not require atmospheric water vapor to cure.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.30 g/cc2.30 g/ccASTM D792
Outgassing - Total Mass Loss 0.40 %0.40 %TML
Collected Volatile Condensable Material 0.18 %0.18 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8585ASTM D2240
Elongation at Break 30 %30 %ASTM D412
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmASTM D257
Dielectric Constant  3.9
@Frequency 100000 Hz
3.9
@Frequency 100000 Hz
ASTM D150
 4.1
@Frequency 100 Hz
4.1
@Frequency 100 Hz
ASTM D150
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear 180 µm/m-°C
@Temperature 20.0 - 105 °C
100 µin/in-°F
@Temperature 68.0 - 221 °F
Thermal Conductivity 0.950 W/m-K6.59 BTU-in/hr-ft²-°FASTM D5470
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Brittleness Temperature -75.0 °C-103 °F
 
Processing PropertiesMetricEnglishComments
Extrusion Rate 0.700 g/min0.700 g/min
Cure Time  60.0 min
@Temperature 100 °C
1.00 hour
@Temperature 212 °F
 240 min
@Temperature 65.0 °C
4.00 hour
@Temperature 149 °F
 300 min
@Temperature 150 °C
5.00 hour
@Temperature 302 °F
 10100 min
@Temperature 25.0 °C
168 hour
@Temperature 77.0 °F
Pot Life 60 min60 min
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-THERM 1641 Thermally Conductive Silicone
Celanese CoolPoly® E8101 Thermally Conductive Thermoplastic Elastomer
Celanese CoolPoly® E5105 Thermally Conductive Polyphenylene Sulfide
Celanese CoolPoly® E5103 Thermally Conductive Polyphenylene Sulfide
Celanese CoolPoly® E4501 Thermally Conductive Polycarbonate

PCHOME176 / 28398

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.