MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® C 50 H2 PA6, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Description: TECHNYL® C 50H2 is a unreinforced melamine cyanurate flame retarded polyamide 6. This product is heat stabilized and can be used for injection molding and extrusion processes. This product is available in natural & black, and in other colors upon request.

Benefits: This product, UL94 VO @ 0,4mm, offers excellent moldability together with good stiffness.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: Connectivity- junction blocks, terminal blocks, connectors…

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183/A
Water Absorption 1.1 %
@Temperature 23.0 °C,
Time 86400 sec
1.1 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.013 cm/cm0.013 in/in
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 60.0 MPa8700 psiISO 527 Type 1A
 80.0 MPa11600 psiASTM D638
Tensile Strength, Yield 75.0 MPa10900 psiISO 527 type 1 A
 80.0 MPa11600 psiASTM D638
Elongation at Break 15 %15 %ASTM D638
 25 %25 %ISO 527 Type 1A
Elongation at Yield 3.5 %3.5 %ISO 527 type 1 A
Tensile Modulus 3.50 GPa508 ksiISO 527 Type 1A
Flexural Strength 115 MPa16700 psiASTM D790
 200 MPa29000 psiISO 178
Flexural Modulus 3.15 GPa457 ksiISO 178
 3.50 GPa508 ksiASTM D790
Izod Impact, Notched 0.650 J/cm1.22 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 3.50 kJ/m²1.67 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 18.0 J/cm²85.7 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 3.53.5IEC 60250
Dielectric Strength 34.0 kV/mm864 kV/inIEC 60243
Dissipation Factor 0.0200.020IEC 60250
Comparative Tracking Index 475 V475 VSolution B; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 222 °C432 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °FISO 75/Af
Flammability, UL94  V-0
@Thickness 0.380 mm
V-0
@Thickness 0.0150 in
1210
 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
1210
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
1210
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
1210
Oxygen Index 36 %36 %ISO 4589
Glow Wire Ignition Temperature  700 °C
@Thickness 0.800 mm
1290 °F
@Thickness 0.0315 in
ISO 60695-2-13
 700 °C
@Thickness 1.60 mm
1290 °F
@Thickness 0.0630 in
ISO 60695-2-13
 700 °C
@Thickness 3.20 mm
1290 °F
@Thickness 0.126 in
ISO 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 230 - 235 °C446 - 455 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone235-245°C
Fire and smoke F indexI2/F3NF F 16 101
Mixing Zone245-250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® C50H2 Nylon 6, Flame Retardant, Heat Stabilized
Celanese Nilit Nilamid B FR HF Unfilled, Flame Retardant, Halogen and Red Phosphorous Free PA6
Avient Bergamid™ B700 UF black Polyamide 6 (Nylon 6), DAM
LATI Latamid 6 H2PX-V0 PA 6, Heat Stabilized, Flame Retardant
Celanese Nilit FRIANYL B63 HS-GV10 Nylon 6 for injection molding, 10% glass fiber reinforced

PRHOD789 / 138020

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.