MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® F161 Epoxy Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: F161 is a structural, heat resistant and electrical grade epoxy formulation designed for autoclave curing. F161 is a high temperature, laminate grade epoxy resin with a 350ºF (177ºC) cure. F161 is unique in that it was the first resin system to meet all types and classes of MIL-R-9300 B.

Uncured: Moderate viscosity during cure, Adaptable to offer good tack and drape for processing, Can be adapted for use on various weaves and fiber reinforcements, Nonburning system available (Bromine added);
Cured: Heat resistant properties, Excellent heat aging properties (adaptable to tooling), Electrical grade formulation, Certified to MIL-R-9300 B (Types 1 and II, Grades O and D, Form B)

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.243 g/cc1.243 g/cc
Moisture Absorption at Equilibrium 2.8 %2.8 %
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 60.0 MPa8700 psi
Elongation at Yield 2.2 %2.2 %
Tensile Modulus 3.59 GPa521 ksi
Fracture Toughness 0.433 MPa-m½0.394 ksi-in½
 
Thermal PropertiesMetricEnglishComments
CTE, linear 46.8 µm/m-°C26.0 µin/in-°F
Glass Transition Temp, Tg 152 °C306 °FWet
 197 °C387 °FDry
 
Processing PropertiesMetricEnglishComments
Gel Time 1.00 - 7.00 min
@Temperature 177 °C
1.00 - 7.00 min
@Temperature 351 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® F155 Epoxy Resin
Master Bond EP112M Two Component, Medium Viscosity Heat Curing Cycloaliphatic Epoxy Resin
Hexcel® HexPly® F155 Epoxy Resin, K120 Kevlar Fabric
Solvay CYCOM® 7701 Epoxy - Crowfoot Satin Fabric Composite
Solvay CYCOM® 7668 Epoxy Resin

PHEXC107 / 98577

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.