MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Arkema Rilsan® MB 3000 NAT Nylon 11, Sheathing Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11); Nylon 11, Cable Sheathing Grade

Material Notes: Designation ISO 1874-PA11,MF,12-010

Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be processed for injection molding and sheathing of cables. Low shrinkage for molding: include 1% on average for the mold design.

UL classification: UL94 V0 (3mm) RTI(C) 65/65/65

Example applications: Electrical cables, all pieces with fireproofing required.

Information provided by Arkema.

Key Words: PA11; Polyamide 11
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
 1.09 g/cc0.0394 lb/in³Cond.; ISO 1183
Water Absorption 2.0 %2.0 %Dry; Sim. to ISO 62
Moisture Absorption 0.600 %0.600 %Dry; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inDry; ISO 294-4, 2577
 0.0090 cm/cm0.0090 in/in
Melt Flow 95 g/10 min
@Load 2.16 kg,
Temperature 235 °C
95 g/10 min
@Load 4.76 lb,
Temperature 455 °F
cm³/10 min Volumetric Rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 69
@Time 15.0 sec
69
@Time 0.00417 hour
Dry; ISO 7619-1
Tensile Strength, Yield 45.0 MPa6530 psiDry; ISO 527-1/-2
 45.0 MPa6530 psiCond.; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %Dry; ISO 527-1/-2
 >= 50 %>= 50 %Cond.; ISO 527-1/-2
Elongation at Yield 5.0 %5.0 %Dry; ISO 527-1/-2
 5.0 %5.0 %Cond.; ISO 527-1/-2
Tensile Modulus 1.83 GPa265 ksiCond.; ISO 527-1/-2
Charpy Impact Unnotched  3.80 J/cm²
@Temperature -30.0 °C
18.1 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eU
 8.30 J/cm²
@Temperature 23.0 °C
39.5 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
Cond.; ISO 179/1eA
 0.400 J/cm²
@Temperature 23.0 °C
1.90 ft-lb/in²
@Temperature 73.4 °F
Cond.; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
 >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmCond.; IEC 60093
Dielectric Constant  3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
Dry; IEC 60250
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Dry; IEC 60250
Dielectric Strength 28.0 kV/mm711 kV/inDry; IEC 60243-1
 28.0 kV/mm711 kV/inCond.; IEC 60243-1
Dissipation Factor  0.018
@Frequency 1e+6 Hz
0.018
@Frequency 1e+6 Hz
Dry; IEC 60250
 0.0221
@Frequency 100 Hz
0.0221
@Frequency 100 Hz
Dry; IEC 60250
Comparative Tracking Index 600 V600 VCond.; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 102 µm/m-°C56.7 µin/in-°FDry; ISO 11359-1/-2
Melting Point 189 °C372 °F10°C/min; Dry; ISO 11357-1/-3
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
Yellow Card Available; Dry; IEC 60695-11-10
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Yellow Card Available; Dry; IEC 60695-11-10
Oxygen Index 33 %33 %Dry; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 °C500 °FInjection Molding; ISO 294
Mold Temperature 50.0 °C122 °FInjection Molding; ISO 10724
Hold Pressure 16.0 MPa2320 psiInjection Molding; ISO 294
 
Descriptive Properties
%Bio-Based90ASTM D6866
Bio-BasedYes
Form as DeliveredPellets
Heat StabilizedYes
Light StabilizedYes
LubricantsYes
Moisture SensitiveYes
Processing MethodsInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Arkema Rilsan® BESNO P40 W6 TL PA11 FR(30)
Arkema Rilsan® BZM 30 O TL PA11-GF30
Clariant Renol PA113G30TF15S2 Nylon 66, 30% Glass Fiber, Teflon and Silicone Lubricated
EMS-Grivory Grilamid® TR 90 PAMACM12
Techmer ES Luriblend® PA11 GF30 TL20 LE 30% Glass Filled

PARKG661 / 25910

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.