MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borstar® FB4250T LLDPE for Blown Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes: Borstar FB4250 is well suited for a wide range of film applications due to its properties. The well balanced mechanical properties will improve the functionality of the films or allow for material saving through down gauging compared to LDPE. Borstar FB4250T is especially well suited for film lines that are limited due to melt pressure. Typical applications are protection films, carrier bags, industrial liners and pouches, pouches, liners, etc. Borstar FB4250T is well suited for coextrusion due to its easy flow properties.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ISO 1183
Thickness 70.0 microns2.76 mil
Melt Flow  0.40 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 2.0 g/10 min
@Load 5.00 kg,
Temperature 190 °C
2.0 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 650 %650 %ISO 527-3
Film Elongation at Break, TD 790 %790 %ISO 527-3
Secant Modulus, MD 0.260 GPa37.7 ksiASTM D882-A
Secant Modulus, TD 0.310 GPa45.0 ksiASTM D882-A
Coefficient of Friction >= 0.50>= 0.50ISO 8295
Tear Strength, Total 4.50 N1.01 lb (f)MD; ISO 6383/3
 15.0 N3.37 lb (f)TD; ISO 6383/2
Dart Drop 3.85 g/micron97.8 g/milISO 7765/1
Film Tensile Strength at Break, MD 38.0 MPa5510 psiISO 527-3
Film Tensile Strength at Break, TD 35.0 MPa5080 psiISO 527-3
 
Optical PropertiesMetricEnglishComments
Haze 20 %20 %ASTM D1003-00
Gloss 70 %70 %ASTM D2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis Borstar® FB2310 LLDPE for Film
Borealis Borstar® FB2230 LLDPE for Film
Borealis Borstar® FB1460 HDPE for Film
Borealis FG5190 Linear Low Density Polyethylene
Borealis Borstar® FB4230 LLDPE for Film

PBOREA114 / 27421

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.