414 Stainless Steel, annealed plate
Categories:
Metal
;
Ferrous Metal
;
Heat Resisting
;
Stainless Steel
;
T 400 Series Stainless Steel
Key Words:
UNS S41400, AMS 5615, ASTM A276, ASTM A314, ASTM A473, ASTM A511, ASTM A580, FED QQ-S-763, SAE J405 (51414), martensitic
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
7.80
g/cc
0.282
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Brinell
235
235
Hardness, Rockwell B
97
97
Converted from Brinell
Hardness, Rockwell C
21
21
Converted from Brinell
Hardness, Vickers
247
247
Converted from Brinell
Tensile Strength, Ultimate
795
MPa
115000
psi
Tensile Strength, Yield
620
MPa
@Strain 0.2 %
89900
psi
@Strain 0.2 %
Elongation at Break
20 %
20 %
in 50 mm
Tensile Modulus
200
GPa
29000
ksi
Izod Impact
30.0
-
80.0
J
22.1
-
59.0
ft-lb
hardened and tempered
70.0
-
110
J
51.6
-
81.1
ft-lb
annealed
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.0000700
ohm-cm
@Temperature 20.0 °C
0.0000700
ohm-cm
@Temperature 68.0 °F
Thermal Properties
Metric
English
Comments
CTE, linear
10.4
µm/m-°C
@Temperature 0.000 - 100 °C
5.78
µin/in-°F
@Temperature 32.0 - 212 °F
11.0
µm/m-°C
@Temperature 0.000 - 315 °C
6.11
µin/in-°F
@Temperature 32.0 - 599 °F
12.1
µm/m-°C
@Temperature 0.000 - 540 °C
6.72
µin/in-°F
@Temperature 32.0 - 1000 °F
12.4
µm/m-°C
@Temperature 0.000 - 650 °C
6.89
µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity
0.460
J/g-°C
@Temperature 0.000 - 100 °C
0.110
BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity
24.9
W/m-K
@Temperature 100 °C
173
BTU-in/hr-ft²-°F
@Temperature 212 °F
28.7
W/m-K
@Temperature 500 °C
199
BTU-in/hr-ft²-°F
@Temperature 932 °F
Melting Point
1425
-
1480
°C
2597
-
2700
°F
Solidus
1425
°C
2597
°F
Liquidus
1480
°C
2700
°F
Component Elements Properties
Metric
English
Comments
Carbon, C
<= 0.15 %
<= 0.15 %
Chromium, Cr
12.5 %
12.5 %
Iron, Fe
83 %
83 %
Manganese, Mn
<= 1.0 %
<= 1.0 %
Nickel, Ni
1.88 %
1.88 %
Phosphorus, P
<= 0.040 %
<= 0.040 %
Silicon, Si
<= 1.0 %
<= 1.0 %
Sulfur, S
<= 0.030 %
<= 0.030 %
References
for this datasheet.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
AISI 4130 Steel, water quenched 855°C (1570°F), 540°C (1000°F) temper, 100 mm (4 in.) round
AISI 6150 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 100 mm (4 in.) round
414 Stainless Steel, annealed and cold drawn bar
308 Stainless steel, cold drawn wire, 25% hardened
AISI 5140 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 25 mm (1 in.) round
MQ414M / 13025
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.