MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Evonik DYNAPOL® S EP1408 Linear Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: A saturated linear copolyester, slightly crystalline. Generally used for solvent based lamination.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity  15000 cP
@Temperature 220 °C
15000 cP
@Temperature 428 °F
melt; (Plate/Plate)
 30000 cP
@Temperature 200 °C
30000 cP
@Temperature 392 °F
melt; (Plate/Plate)
 55000 cP
@Temperature 180 °C
55000 cP
@Temperature 356 °F
melt; (Plate/Plate)
 100000 cP
@Temperature 160 °C
100000 cP
@Temperature 320 °F
melt; (Plate/Plate)
Viscosity Test 90 cm³/g0.90 dl/gDIN 53 728
Melt Flow  75 g/10 min
@Temperature 160 °C
75 g/10 min
@Temperature 320 °F
DIN ISO 1133
 130 g/10 min
@Temperature 180 °C
130 g/10 min
@Temperature 356 °F
DIN ISO 1133
 200 g/10 min
@Temperature 200 °C
200 g/10 min
@Temperature 392 °F
DIN ISO 1133
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 2.02.0
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 1717
Tensile Strength, Ultimate 2.00 MPa290 psiDIN EN ISO 527-1/3
Elongation at Break 500 %500 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 80.0 °C176 °FDIN 53 765
Softening Point 95.0 °C203 °FDIN ISO 4625
Glass Transition Temp, Tg -30.0 °C-22.0 °FDIN 53 765
 
Descriptive Properties
Hydroxyl Number (mg KOH/g)4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SK Chemicals SKYTHANE® SG200 SKYGREEN Biodegradable Thermoplastic
SK Chemicals SKYTHANE® T865A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
SK Chemicals SKYTHANE® T850A Polyester Based, Low Hardness Thermoplastic Polyurethane Elastomer
SK Chemicals SKYTHANE® SG400 SKYGREEN Biodegradable Thermoplastic
SK Chemicals SKYTHANE® S375D Polyester Based Thermoplastic Polyurethane Elastomer

PHUMB282 / 81284

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.