Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important properties:- High melt strength
- Impact resistant even at low temperatures
- Easy processing
- Processable on conventional as well as on 3 D-machines
- Suitable for sequential blow molding process in combination with flexible grades
Grilon EBV-15H black 9697 is used typically for automotive applications such are air ducts for turbo-chargers, air ducts, oil filler pipes, fuel and oil containers.Information provided by EMS Grivory. |