MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MRC Polymers NAXELL™ PC110-20G General Purpose Medium Viscosity Polycarbonate 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Glass Fiber Filled, Flame Retardant

Material Notes: General Purpose Medium Viscosity Polycarbonate 20% Glass Fiber Reinforced

Mechanical properties measured on 1/8 in. (3.2 mm) samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
@Thickness 3.17 mm
0.0010 - 0.0030 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 103 MPa14900 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Flexural Yield Strength 131 MPa19000 psiASTM D790
Flexural Modulus 5.168 GPa749.6 ksiASTM D790
Izod Impact, Notched 1.068 J/cm2.001 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.0 µm/m-°C
@Temperature -40.0 - 35.0 °C
15.0 µin/in-°F
@Temperature -40.0 - 95.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 146 °C295 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 141 °C286 °FUnannealed; ASTM D648
Flammability, UL94  V-1
@Thickness 1.47 mm
V-1
@Thickness 0.0579 in
MRC Rating
 V-1
@Thickness 1.47 mm
V-1
@Thickness 0.0579 in
MRC Rating
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
MRC Rating
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
MRC Rating
 
Processing PropertiesMetricEnglishComments
Processing Temperature 299 - 343 °C570 - 649 °F
Rear Barrel Temperature 299 - 332 °C570 - 630 °F
Middle Barrel Temperature 304 - 338 °C579 - 640 °F
Front Barrel Temperature 316 - 343 °C601 - 649 °F
Nozzle Temperature 316 - 338 °C601 - 640 °F
Mold Temperature 66.0 - 116 °C151 - 241 °F
Drying Temperature 138 - 149 °C280 - 300 °F
Dry Time 4 - 6 hour4 - 6 hour
Moisture Content <= 0.020 %<= 0.020 %
Dew Point <= -17.8 °C<= 0.000 °F
Drying Air Flow Rate 22.7 - 28.3 l/min0.800 - 1.00 ft³/min (CFM)per lb/hour resin processed
Injection Pressure 68.9 - 138 MPa10000 - 20000 psi
Back Pressure 0.000 - 0.517 MPa0.000 - 75.0 psi
Cushion 0.635 cm0.250 in
Screw Speed 30 - 75 rpm30 - 75 rpm
 
Descriptive Properties
Fill RateModerate
Hold Pressure40 - 60% of injection pressure
Packing Pressure50 - 75% of injection pressure

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MRC Polymers NAXELL™ PC110-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Medium Viscosity
MRC Polymers NAXELL™ PC23M-20G General Purpose Low Viscosity Polycarbonate 20% Glass Fiber Reinforced
MRC Polymers NAXELL™ PC23M-10G General Purpose Polycarbonate, 10% Glass Fiber Filled, Low Viscosity
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose
MRC Polymers NAXELL™ PC110-30G General Purpose Medium Viscosity Polycarbonate 30% Glass Fiber Reinforced

PMRC958 / 21025

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.