MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dynasol Solprene® 9618 Multi-branched Thermoplastic Rubber (Multi-branched SBS)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: Solprene 9618 is a 69/31 Butadiene-Styrene multi arm copolymer, polymerized in solution process. It is stabilized with non-staining antioxidant system. This product is presented as a free flowing porous pellet for easy handling and dissolution.

Uses: Solprene 9618 is designed to be used in high performance adhesive formulations.

Main Applications:
Adhesives
Polymer modification

Information provided by Dynasol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 0.75 %<= 0.75 %ASTM D5668
Brookfield Viscosity 0.60 cP0.60 cP25% in toluene; ASTM D2994
Melt Flow 13 g/10 min13 g/10 minASTM D1238
 
Chemical PropertiesMetricEnglishComments
Styrene Content 29 %29 %Block; NM 202-07
 31 %31 %NM 300-14
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7575DIN 53505
Tensile Strength 8.00 MPa1160 psiASTM D412
Elongation at Break 850 %850 %ASTM D412
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -66.0 °C-86.8 °FASTM E-1356

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dynasol Solprene® 4302 Thermoplastic Rubber (SBS)
Dynasol Solprene® 4321 Thermoplastic Rubber (SBS)
Dynasol Solprene® 4316 Thermoplastic Rubber (SBS)
Dynasol Solprene® 4301 Thermoplastic Rubber (SBS)
Dynasol Solprene® 4318 Thermoplastic Rubber SBS Dry

PDYNA993 / 132988

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.