MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Tra-Con Tra-Bond 2158 Heat Conductive Electrically Insulating Compound
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: TRA-BOND 2158 is a flexible, thermal conductive epoxy system. It is used for staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards. This two-part adhesive develops strong, durable, high-impact bonds at room temperature which improve heat transfer while maintaining electrical insulation. TRA-BOND 2158 bonds readily to itself, and to metals, silica, steatite, alumina, sapphire and other ceramics, glass, plastics and many other materials, because its coefficient of thermal expansion provides a good match for those materials over a fairly wide temperature range. Fully cured TRA-BOND 2158 provides excellent resistance to salt solutions, mild acids and alkalis, and many other chemicals including petroleum solvents, lubricating oils, and alcohol.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.30 g/cc2.30 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
Viscosity 15000 cP
@Temperature 25.0 °C
15000 cP
@Temperature 77.0 °F
After mixing
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.10e+15 ohm-cm2.10e+15 ohm-cm
 3.20e+13 ohm-cm
@Temperature 75.0 °C
3.20e+13 ohm-cm
@Temperature 167 °F
Dielectric Constant 5.9
@Frequency 1000 Hz
5.9
@Frequency 1000 Hz
Dielectric Strength 16.1 kV/mm410 kV/in
Dissipation Factor 0.010
@Frequency 1000 Hz
0.010
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.840 W/m-K5.83 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 240 min
@Temperature 65.0 °C
2.00 - 4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 180 min180 min
 
Descriptive Properties
Color Tan
Mix Ratio, parts by weight100/38Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond 2156 Heat Conductive Electrically Insulating Compound
Tra-Con Tra-Bond 2159 Heat Conductive Electrically Insulating Compound
Tra-Con Tra-Bond 2151 Thermally Conductive Electrically Insulating Compound
Tra-Con Tra-Bond 2151T Thermally Conductive Electrically Insulating Compound
Tra-Con Tra-Bond 2152 Thermally Conductive Electrically Insulating Compound

PTRAC039 / 70967

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.