MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 9840 Steel, 540°C (1000°F) temper, 25 mm (1 in.) round
Categories: Metal; Ferrous Metal; Alloy Steel; AISI 9000 Series Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Quenched, 540°C temper, 525°C nitride for 40 hours with 20-30% ammonia dissociation, hardness of 88 HR15N case hardness at 0.635-0.762 mm nitrided case depth

Key Words: UNS G98400, AMS 6342 C, ASTM A274, ASTM A322, ASTM A519, SAE J778, DIN 1.6511, UNI 38 NiCrMo 4, B.S. 816 M 40
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³field average for steels
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 361361
Hardness, Knoop 390390Converted from Brinell
Hardness, Rockwell B 100100Converted from Brinell
Hardness, Rockwell C 3535core hardness. Quenched, 540°C temper, 525°C nitride for 40 hours with 20-30% ammonia dissociation
Hardness, Vickers 382382Converted from Brinell
Tensile Strength, Ultimate 1240 MPa180000 psi
Tensile Strength, Yield 1105 MPa160300 psi
Elongation at Break 15 %15 %in 50 mm
Modulus of Elasticity 200 GPa29000 ksiEstimated
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Calculated
Machinability 70 %70 %Estimated
Shear Modulus 80.0 GPa11600 ksiTypical for steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000174 ohm-cm0.0000174 ohm-cmEstimated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 20.0 °C
6.39 µin/in-°F
@Temperature 68.0 °F
 12.2 µm/m-°C
@Temperature 250 °C
6.78 µin/in-°F
@Temperature 482 °F
Estimated
 13.9 µm/m-°C
@Temperature 500 °C
7.72 µin/in-°F
@Temperature 932 °F
 14.7 µm/m-°C
@Temperature 1000 °C
8.17 µin/in-°F
@Temperature 1830 °F
Specific Heat Capacity 0.472 J/g-°C0.113 BTU/lb-°FEstimated
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.38 - 0.43 %0.38 - 0.43 %
Chromium, Cr 0.70 - 0.90 %0.70 - 0.90 %
Iron, Fe 95.945 - 97.02 %95.945 - 97.02 %As remainder
Manganese, Mn 0.70 - 0.90 %0.70 - 0.90 %
Molybdenum, Mo 0.20 - 0.30 %0.20 - 0.30 %
Nickel, Ni 0.85 - 1.15 %0.85 - 1.15 %
Phosphorus, P <= 0.035 %<= 0.035 %
Silicon, Si 0.15 - 0.30 %0.15 - 0.30 %
Sulfur, S <= 0.040 %<= 0.040 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 9840 Steel, 595°C (1100°F) temper, 25 mm (1 in.) round
AISI 9840 Steel, 650°C (1200°F) temper, 25 mm (1 in.) round
AISI 1040 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
AISI 1040 Steel, as cold drawn, 50-75 mm (2-3 in) round
AISI 4340 Steel, oil quenched 800°C (1470°F), 540°C (1000°F) temper, 25 mm round

M984AA / 8711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.