MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Aluminum 7175-T66
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A97175; Aluminium 7175-T66; AA7175-T66; Al7175-T66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.80 g/cc0.101 lb/in³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 150150500 kg load with 10 mm ball
Hardness, Knoop 191191Converted from Brinell Hardness Value
Hardness, Rockwell A 53.553.5Converted from Brinell Hardness Value
Hardness, Rockwell B 8686Converted from Brinell Hardness Value
Hardness, Vickers 170170Converted from Brinell Hardness Value
Tensile Strength, Ultimate 590 MPa85600 psi
Tensile Strength, Yield 520 MPa75400 psi
Elongation at Break 11 %11 %In 5 cm; Sample 1.6 mm thick
Tensile Modulus 72.0 GPa10400 ksiCompressive Modulus is about 2% higher
Poissons Ratio 0.330.33Estimated from trends in similar Al alloys.
Fatigue Strength 160 MPa
@# of Cycles 5.00e+8
23200 psi
@# of Cycles 5.00e+8
Shear Modulus 27.0 GPa3920 ksiEstimated from similar Al alloys.
Shear Strength 350 MPa50800 psiCalculated value.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000479 ohm-cm0.00000479 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  21.6 µm/m-°C
@Temperature -50.0 - 20.0 °C
12.0 µin/in-°F
@Temperature -58.0 - 68.0 °F
 23.4 µm/m-°C
@Temperature 20.0 - 100 °C
13.0 µin/in-°F
@Temperature 68.0 - 212 °F
AA; Typical; average over range
 24.3 µm/m-°C
@Temperature 20.0 - 200 °C
13.5 µin/in-°F
@Temperature 68.0 - 392 °F
 25.2 µm/m-°C
@Temperature 20.0 - 300 °C
14.0 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.864 J/g-°C0.207 BTU/lb-°F
Thermal Conductivity 142 W/m-K985 BTU-in/hr-ft²-°F
Melting Point 477 - 635.0 °C890 - 1175 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Homogenization may raise eutectic melting temperature 20-40°F but usually does not eliminate it.
Solidus 477 °C890 °FAA; Typical
Liquidus 635.0 °C1175 °FAA; Typical
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 413 °C775 °F
Solution Temperature 516 °C960 °Fmust be preceded by soak at 890 to 905°F; quench from lower temperature
Aging Temperature 121 - 177 °C250 - 350 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 88 - 91.4 %88 - 91.4 %As remainder
Chromium, Cr 0.18 - 0.28 %0.18 - 0.28 %
Copper, Cu 1.2 - 2.0 %1.2 - 2.0 %
Iron, Fe <= 0.20 %<= 0.20 %
Magnesium, Mg 2.1 - 2.9 %2.1 - 2.9 %
Manganese, Mn <= 0.10 %<= 0.10 %
Other, each <= 0.05 %<= 0.05 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.15 %<= 0.15 %
Titanium, Ti <= 0.10 %<= 0.10 %
Zinc, Zn 5.1 - 6.1 %5.1 - 6.1 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 7068-T6; 7068-T6511 Rod & Bar
Aluminum 6351-T6; 6351-T651
Aluminum 6082-T6
Aluminum 7075-T6; 7075-T651
Aluminum 7001-T6; 7001-T651

MA7175T66 / 9613

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.