MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Medalist® MD-12130 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-12100 Series are high performance thermoplastic elastomer designed for use in healthcare and medical applications requiring high elasticity and excellent moldability. Medalist MD-12130 is a low hardness, low density grade, available in NAT and colors, which can be sterilizable and exhibits excellent adhesion to polypropylene.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability; Good Flexibility; Good Moldability; Good Sterilizable; Good Toughness; Halogen Free; Low Density; Low Flow; Low Hardness; Low Specific Gravity; Radiation Sterilizable; Radiation (Gamma) Resistant; Resilient; Slip; Without Fillers

Uses: Bushings; Connectors; Flexible Grips; Gaskets; Grommets; Handles; Knobs; Medical/Healthcare Applications; Overmolding; Pharmaceuticals; Rubber Replacement; Seals; Soft Touch Applications

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Preliminary data.

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.883 g/cc0.0319 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
2.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  30
@Time 5.00 sec
30
@Time 0.00139 hour
ASTM D2240
 32
@Time 1.00 sec
32
@Time 0.000278 hour
ASTM D2240
Tensile Strength at Break 2.79 MPa405 psiDie C, 20 in/min; ASTM D412
Tensile Stress at Strain  0.827 MPa
@Strain 50 %
120 psi
@Strain 50 %
Die C, 20 in/min; ASTM D412
 1.03 MPa
@Strain 100 %
150 psi
@Strain 100 %
Die C, 20 in/min; ASTM D412
 1.65 MPa
@Strain 300 %
240 psi
@Strain 300 %
Die C, 20 in/min; ASTM D412
Elongation at Break 540 %540 %Die C, 20 in/min; ASTM D412
Tear Strength 12.1 kN/m69.0 pliDie C, 20 in/min; ASTM D624
Compression Set  13 %
@Temperature 22.8 °C,
Time 79200 sec
13 %
@Temperature 73.0 °F,
Time 22.0 hour
Type 1; ASTM D395B
 20 %
@Temperature 70.0 °C,
Time 79200 sec
20 %
@Temperature 158 °F,
Time 22.0 hour
Type 1; ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 160 - 177 °C320 - 350 °F
Middle Barrel Temperature 182 - 204 °C360 - 400 °F
Front Barrel Temperature 193 - 216 °C380 - 420 °F
Nozzle Temperature 182 - 227 °C360 - 440 °F
Melt Temperature 182 - 227 °C360 - 440 °F
Mold Temperature 26.7 - 48.9 °C80.0 - 120 °F
Back Pressure 0.345 - 1.03 MPa50.0 - 150 psi
Cushion 0.381 - 2.54 cm0.150 - 1.00 in
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Translucent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Medalist® MD-305 Thermoplastic Elastomer
Teknor Apex Medalist® MD-300 Thermoplastic Elastomer
Teknor Apex Medalist® MD-210 Thermoplastic Elastomer
Teknor Apex Medalist® MD-205 Thermoplastic Elastomer
Teknor Apex Medalist® MD-12170 Thermoplastic Elastomer

PTEKNQ0680 / 237171

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.