MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Quantum Composites AMC™ 8593 NT 50% Carbon Fiber Reinforced SMC
Categories: Polymer; Thermoset; Composite SMC; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: AMC™ 8593 NT is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat resistance and a low density. The carbon fiber is a standard modulus PAN based 3K tow.

  • Form = Rolled Sheet
  • Color = Black or Natural
  • Carbon Fiber Content = Nominal - 50% w/w
  • Resin Content = Nominal 50% w/w

A. Schulman has acquired Quantum Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.47 g/cc1.47 g/ccASTM D792
Linear Mold Shrinkage <= 0.00 cm/cm<= 0.00 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 421 MPa61100 psiASTM D638
Flexural Strength 792 MPa115000 psiASTM D790
Flexural Modulus 44.7 GPa6480 ksiASTM D790
Izod Impact, Notched 10.68 J/cm20.01 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 287 °C549 °FDeflection Temperature, Load not specified; ASTM D648
Glass Transition Temp, Tg 118 °C244 °FASTM D4065
 
Processing PropertiesMetricEnglishComments
Processing Temperature 127 - 154 °C260 - 310 °FCompression Molding
Cure Time 5.00 - 10.0 min
@Temperature 138 °C
0.0833 - 0.167 hour
@Temperature 280 °F
Shelf Life 2.00 Month
@Temperature 23.9 °C
2.00 Month
@Temperature 75.0 °F
 
Descriptive Properties
Fiber Length (in)1Carbon, nominal

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Quantum Composites LYTEX® 4181 55% Carbon Fiber Reinforced Epoxy SMC
Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC
Epoxy Novolac 27%, Carbon fabric 73%
Solvay Thornel® P-55 Carbon Fiber/Epoxy Advanced Composite System
Overview of materials for Epoxy/Carbon Fiber Composite

PCOQB908 / 139276

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.