MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zytel® HTN51G35HSLR BK420 PA6T/XT-GF35
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 40% Glass Fiber Filled

Material Notes: 35% Glass Reinforced, PPA, High Performance Polyamide

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³DAM; ISO 1183
Water Absorption 4.0 %
@Thickness 2.00 mm
4.0 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 1.40 %
@Thickness 2.00 mm
1.40 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 310 MPa45000 psiH 961/30; DAM; ISO 2039-1
Tensile Strength at Break 190 MPa27600 psi50% RH; ISO 527-1/-2
 200 MPa29000 psiDAM; ISO 527-1/-2
Elongation at Break 2.0 %2.0 %50% RH; ISO 527-1/-2
 2.3 %2.3 %DAM; ISO 527-1/-2
Tensile Modulus 12.0 GPa1740 ksi50% RH; ISO 527-1/-2
 12.0 GPa1740 ksiDAM; ISO 527-1/-2
Flexural Modulus 10.5 GPa1520 ksiDAM; ISO 178
Poissons Ratio 0.330.3350% RH
 0.330.33DAM
Charpy Impact Unnotched  4.00 J/cm²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 5.00 J/cm²
@Temperature 23.0 °C
23.8 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 0.900 J/cm²
@Temperature 23.0 °C
4.28 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmDAM; IEC 62631-3-1
Dielectric Strength 33.0 kV/mm838 kV/in50% RH; IEC 60243-1
 34.0 kV/mm864 kV/inDAM; IEC 60243-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FDAM; ISO 11359-1/-2
 20.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
11.1 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 58.0 µm/m-°C32.2 µin/in-°FDAM; ISO 11359-1/-2
 55.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
30.6 µin/in-°F
@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
Melting Point 300 °C572 °Ffirst heat; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 276 °C529 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 262 °C504 °FDAM; ISO 75-1/-2
Glass Transition Temp, Tg 95.0 °C203 °F10°C/min; 50% RH; ISO 11357-1/-2
 135 °C275 °F10°C/min; DAM; ISO 11357-1/-2
Flame Spread 28.0 mm/min
@Thickness 1.00 mm
1.10 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 325 °C617 °FOptimum, Injection
 320 - 330 °C608 - 626 °FRange, Injection
Mold Temperature 150 °C302 °FOptimum, Injection
 140 - 180 °C284 - 356 °FInjection; higher temperature needed for thinner sections
Drying Temperature 100 °C212 °FInjection
Dry Time 6.00 - 8.00 hour6.00 - 8.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.10 %<= 0.10 %Injection
 
Descriptive Properties
AdditivesRelease agent
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
ISO designationISO 16396-PA6T/XT,GF35,M1CGHRW,S10-120
Odor Class4VDA 270
Part Marking Code>PA6T/XT-GF35<ISO 11469
 >PPA-GF35<SAE J1344
PolymerPA6T/XT-GF35
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA6T/XT-GF35ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® HTN51G35HSL NC010 PA6T/XT-GF35
Celanese Zytel® HTN51G35HSLR BK420J PA6T/XT-GF35
Celanese Zytel® HTN51G35EF BK083 PA6T/XT-GF35
Celanese Zytel® HTN51G35HSL BK083 PA6T/XT-GF35
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)

PDSX5436 / 198076

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.