MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® 6406 PBT, 40% Mineral / Glass Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Glass + Mineral Filled

Material Notes: Celanex 6406 is a 40% mineral/glass reinforced resin providing excellent toughness combined with warpage resistance, surface gloss and good mechanical properties. Celanex 6406 is particularly suited to applications requiring flatness and good surface appe
To avoid hydrolytic degradation during processing, CELANEX resins have to be dried to a moisture level equal to or less than 0.02%. Drying should be done in a dehumidifying hopper dryer capable of dewpoints <-40°F (-40°C) at 250°F (121°C) for 4 hours.
For subsequent storage of the material in the dryer until processed (<= 60 h) it is necessary to lower the temperature to 100° C.

Information provided by Celanese Corporation.

Key Words: 40% glass/mineral, low warp, improved impact
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/ccASTM D792
Density 1.58 g/cc0.0571 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C/50%RH; ISO 62
Viscosity Test 90 cm³/g0.90 dl/gISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inASTM D955
 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inISO 294-4
Melt Flow 16 g/10 min16 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 5151ISO 2039-2
Tensile Strength at Break 75.0 MPa10900 psi5mm/min; ISO 527-2/1A
 79.3 MPa
@Temperature 22.8 °C
11500 psi
@Temperature 73.0 °F
ASTM D638
Elongation at Break 2.5 %2.5 %5mm/min; ISO 527-2/1A
 3.2 %
@Temperature 22.8 °C
3.2 %
@Temperature 73.0 °F
ASTM D638
Tensile Modulus 7.80 GPa1130 ksi1mm/min; ISO 527-2/1A
Flexural Strength 120 MPa17400 psiISO 178
 110 MPa
@Temperature 22.8 °C
16000 psi
@Temperature 73.0 °F
ASTM D790
Flexural Modulus 7.00 GPa1020 ksiISO 178
 6.62 GPa
@Temperature 22.8 °C
960 ksi
@Temperature 73.0 °F
ASTM D790
Izod Impact, Notched 1.07 J/cm
@Temperature 22.8 °C
2.00 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Notched (ISO) 11.7 kJ/m²5.57 ft-lb/in²ISO 180/1A
 8.00 kJ/m²
@Temperature 30.0 °C
3.81 ft-lb/in²
@Temperature 86.0 °F
ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
@Temperature 23.0 °C
19.0 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact, Notched 1.21 J/cm²5.76 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.80e+14 ohm-cm2.80e+14 ohm-cmASTM D257
Dielectric Constant 4.4
@Frequency 1e+6 Hz
4.4
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 18.5 kV/mm470 kV/inshort term; ASTM D149
Dissipation Factor 0.026
@Frequency 1e+6 Hz
0.026
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 129 sec129 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 97.0 µm/m-°C53.9 µin/in-°FISO 11359-2
Melting Point 225 °C437 °FISO 11357-1,-2,-3
 225 °C437 °FASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 205 °C401 °FISO 75-1, -2
 209 °C408 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 160 °C320 °FISO 75-1, -2
 160 °C320 °FASTM D648
Vicat Softening Point 150 °C302 °FB50 (50°C/h 50N); ISO 306
Flammability, UL94 HBHB
 HB
@Thickness 0.850 mm
HB
@Thickness 0.0335 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 20.0 - 50.0 °C68.0 - 122 °Fhopper
 65.0 - 96.0 °C149 - 205 °Fcavity
Feed Temperature 230 - 250 °C446 - 482 °F
Zone 1 230 - 250 °C446 - 482 °F
Zone 2 235 - 255 °C455 - 491 °F
Zone 3 235 - 255 °C455 - 491 °F
Zone 4 240 - 265 °C464 - 509 °F
Die Temperature 240 - 265 °C464 - 509 °F
Melt Temperature 235 - 265 °C455 - 509 °F
 260 °C500 °FISO 294
Mold Temperature 82.0 °C180 °FISO 294
Injection Velocity 300 mm/sec11.8 in/secISO 294
Drying Temperature 120 - 130 °C248 - 266 °F
Dry Time 4 hour4 hour
Moisture Content 0.020 %0.020 %Necessary low maximum
Injection Pressure 48.0 MPa6960 psiISO 294
Hot-Working Temperature 250 - 265 °C482 - 509 °F
 
Descriptive Properties
Injection moldingYes
Injection speedmedium-fast
Melt volume rate (MVR), cm³/10min16
MVR test load, kg2.16
MVR test temperature, °C265
Processing conditions acc. ISO7792-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Pocan® DP T 7140 LDS 000000 PET + PBT, 42% Glass Fiber/Mineral
Envalior Pocan® T 7141 000000 PET+PBT, 40% Glass Fiber Reinforced
Kraton® FG1901 + PET blend (20/80)
Celanese Zytel® 73G50HSLA BK416 PA6-GF50
Celanese Zytel® 73G45L NC010 PA6-GF45

PHCS088 / 123503

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.