MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Nylon

Nylacast Nylube MO Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), MoS2 Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, MoS2 Filled

Material Notes: The combined Nylube lubrication system incorporating fine particles of molybdenum disulphide provides enhanced load bearing capabilities while retaining Nylube's excellent frictional characteristics.

Information provided by Nylacast Ltd.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.145 g/cc0.04137 lb/in³method A; ISO 1183:1987
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ISO 868:2003
Tensile Strength 85.0 MPa12300 psiType 1B, 50mm/min; ISO 527-1/2:1993
Elongation at Break >= 20 %>= 20 %Type 1B, 50mm/min; ISO 527-1/2:1993
Tensile Modulus 4.20 GPa609 ksiType 1B, 50mm/min; ISO 527-1/2:1993
Flexural Strength 110 MPa16000 psi1.5mm/min; ISO 178:2001
Flexural Modulus 3.50 GPa508 ksi1.5mm/min; ISO 178:2001
Compressive Strength 100 MPa14500 psiType B, 5mm/min; ISO 604:2002
Compressive Modulus 2.80 GPa406 ksiType B, 5mm/min; ISO 604:2002
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²Type A; ISO 180:2000
Coefficient of Friction, Dynamic 0.12
@Pressure 1.75 MPa
0.12
@Pressure 254 psi
31.4m/min
K (wear) Factor 91.0 x 10-8 mm³/N-M
@Pressure 1.75 MPa
45.2 x 10-10 in³-min/ft-lb-hr
@Pressure 254 psi
31.4m/min
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 5.00e+15 ohm-cm5.00e+15 ohm-cmIEC 60093:1980-01
Surface Resistance 5.00e+12 ohm5.00e+12 ohmIEC 60093:1980-01
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 60250:1969-01
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250:1969-01
Dielectric Strength 29.0 kV/mm737 kV/inIEC 60243-1:1998-01
Comparative Tracking Index 604 V604 VIEC 60112:2003-01
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-2:1999
Maximum Service Temperature, Air 185 °C365 °FIntermittent
 115 °C
@Time 1.80e+7 sec
239 °F
@Time 5000 hour
Continuous
Minimum Service Temperature, Air -100 °C-148 °FIntermittent
 -40.0 °C-40.0 °FContinuous
Flammability, UL94 HBHB
 
Descriptive Properties
ColorBlack
Wear Rate0.08 mg/km31.4m/min, 1.75MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nylacast Nylube Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant)
Nylacast Oilon Cast Nylon 6, Lubricated (Lubricant Oil Filled)
Overview of materials for Nylon 6, MoS2 Filled
Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled

PNYLAC09 / 89267

Nylon

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.