MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 221 PA66, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66)

Material Notes: Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors.

Benefits: The product offers a good combination between primary properties of the unreinforced polyamide 66 and processing properties leading to increased productivity. These performances are associated with excellent dimensional stability and good rigidity of molded parts.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: Connectors, lighters, aerosol valves…

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183/A
Water Absorption 1.1 %
@Temperature 23.0 °C,
Time 86400 sec
1.1 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Viscosity  17 cP
@Shear Rate 1000 1/s,
Temperature 300 °C
17 cP
@Shear Rate 1000 1/s,
Temperature 572 °F
 19 cP
@Shear Rate 1000 1/s,
Temperature 290 °C
19 cP
@Shear Rate 1000 1/s,
Temperature 554 °F
 20 cP
@Shear Rate 1000 1/s,
Temperature 280 °C
20 cP
@Shear Rate 1000 1/s,
Temperature 536 °F
 150 cP
@Shear Rate 100 1/s,
Temperature 300 °C
150 cP
@Shear Rate 100 1/s,
Temperature 572 °F
 201 cP
@Shear Rate 100 1/s,
Temperature 280 °C
201 cP
@Shear Rate 100 1/s,
Temperature 536 °F
 201 cP
@Shear Rate 10 1/s,
Temperature 300 °C
201 cP
@Shear Rate 10 1/s,
Temperature 572 °F
 205 cP
@Shear Rate 10 1/s,
Temperature 290 °C
205 cP
@Shear Rate 10 1/s,
Temperature 554 °F
 208 cP
@Shear Rate 100 1/s,
Temperature 290 °C
208 cP
@Shear Rate 100 1/s,
Temperature 554 °F
 220 cP
@Shear Rate 10 1/s,
Temperature 280 °C
220 cP
@Shear Rate 10 1/s,
Temperature 536 °F
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inIsotropy
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/in
Linear Mold Shrinkage, Transverse 0.012 cm/cm0.012 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.0 MPa13800 psiISO 527 Type 1A
 98.0 MPa14200 psiASTM D638
Tensile Stress at Strain  35.0 MPa
@Strain 1 %
5080 psi
@Strain 1 %
 70.0 MPa
@Strain 2 %
10200 psi
@Strain 2 %
 85.0 MPa
@Strain 3 %
12300 psi
@Strain 3 %
 90.0 MPa
@Strain 4 %
13100 psi
@Strain 4 %
Elongation at Break 15 %15 %ASTM D638
 35 %35 %ISO 527 Type 1A
Tensile Modulus 3.20 GPa464 ksiISO 527 Type 1A
Flexural Strength 125 MPa18100 psiISO 178
 125 MPa18100 psiASTM D790
Flexural Modulus 3.15 GPa457 ksiISO 178
 3.20 GPa464 ksiASTM D790
Izod Impact, Notched (ISO) 80.0 kJ/m²38.1 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched NBNBISO 179/1eU
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Constant 2.92.9IEC 60250
Dielectric Strength 27.0 kV/mm686 kV/inIEC 60243
Dissipation Factor 0.0300.030IEC 60250
Comparative Tracking Index 500 V500 VSolution B; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C176 °FASTM D648
 90.0 °C194 °FISO 75/Af
Flammability, UL94  V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
1210
 V-2
@Thickness 1.60 mm
V-2
@Thickness 0.0630 in
1210
Oxygen Index 26 %26 %ISO 4589
Glow Wire Flammability Index 700 °C1290 °FISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 265 - 275 °C509 - 527 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone270-280°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 221 Natural FA PA66, DRY
Domo TECHNYL® A 205F PA66, DRY
Radici Radilon® N66-AFR Nylon 66
Avient Trilliant™ HC THC-02 1200 IL Natural Polyamide 66 (Nylon 66)
Omnia Plastica Akulon® PA 66 - Akulon 66 - Dry

PRHOD685 / 137916

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.