MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Toyobo Vylopet® EMC430 PET/PBT Blend
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polyethylene Terephthalate (PET)

Material Notes: Key Feature: HB UL-94 Class

Applications: general and high rigidity components

PET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and tracking resistance, chemical & weather resistance, and processability.

Information provided by Toyobo Co., Ltd

Key Words: Polyethylene Terephthalate Polyester; Polybutylene Terephthalate; Toyobo Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ASTM D792
Water Absorption 0.050 %0.050 %ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Tensile Strength, Ultimate 118 MPa17100 psiASTM D638
Elongation at Break 2.4 %2.4 %ASTM D638
Flexural Yield Strength 177 MPa25700 psiASTM D790
Flexural Modulus 8.30 GPa1200 ksiASTM D790
Compressive Yield Strength 98.0 MPa14200 psiASTM D695
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
Taber Abrasion, mg/1000 Cycles 3030ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Strength 25.0 kV/mm
@Thickness 2.00 mm
635 kV/in
@Thickness 0.0787 in
ASTM D149
Arc Resistance 122 sec122 secASTM D495
Comparative Tracking Index 260 V260 VIEC test
 
Thermal PropertiesMetricEnglishComments
Melting Point 255 °C491 °FDSC
Deflection Temperature at 0.46 MPa (66 psi) 225 °C437 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C410 °FASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman SCHULADUR® A GF30 30% Glass Fiber Reinforced PBT
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT
Envalior Arnite® TV4 261 PBT-GF30, 30% Glass Filled
Entec Hylox® 9030 PBT, 30% Glass Reinforced
BASF Ultradur® B 4300 G6 30% Glass Filled PBT

PTOY54 / 70726

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.