MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

NOVA Chemicals Sclair® FG220-A Octene LLDPE Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade

Material Notes:

Features:

  • Exceptional toughness
  • Low gel level
  • Applications:

  • Cast stretch wrap
  • Netting
  • Co-extrusion and lamination
  • Information provided by Nova Chemicals

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.920 g/cc0.0332 lb/in³ASTM D792
    Thickness 20.0 microns0.787 mil
    Melt Flow 2.3 g/10 min
    @Load 2.16 kg,
    Temperature 190 °C
    2.3 g/10 min
    @Load 4.76 lb,
    Temperature 374 °F
    ASTM D1238
     
    Mechanical PropertiesMetricEnglishComments
    Film Tensile Strength at Yield, MD 8.89 MPa1290 psiASTM D882
    Film Tensile Strength at Yield, TD 8.41 MPa1220 psiASTM D882
    Film Elongation at Yield, MD 435 %435 %ASTM D638
    Film Elongation at Yield, TD 760 %760 %ASTM D882
    Puncture Energy 1.60 J1.18 ft-lbLow Friction Puncture
    Elmendorf Tear Strength MD 290 g290 gASTM D1922
    Elmendorf Tear Strength TD 650 g650 gASTM D1922
    Dart Drop Test 190 g0.419 lbASTM D1709/A
    Film Tensile Strength at Break, MD 33.0 MPa4790 psiASTM D882
    Film Tensile Strength at Break, TD 25.0 MPa3630 psiASTM D882
    1% Secant Modulus, MD 140.0 MPa20310 psiASTM D882
    1% Secant Modulus, TD 160.0 MPa23210 psiASTM D882
     
    Optical PropertiesMetricEnglishComments
    Haze 2.0 %2.0 %ASTM D1003
    Gloss 85 %85 %at 45°; ASTM D2457

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    NOVA Chemicals Sclair® 11J1 Octene LLDPE Film Resin
    NOVA Chemicals Sclair® FP120-D Octene LLDPE Film Resin
    NOVA Chemicals Sclair® 11J4 Octene LLDPE Film Resin
    NOVA Chemicals Sclair® FP026-F Octene LLDPE Film Resin
    NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin

    PNOV923 / 54869

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.