MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum Nitride, AlN
Categories: Ceramic; Nitride; Other Engineering Material; Semiconductor

Key Words: Pnictide; Semiconductor; Aluminium Nitride
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.26 g/cc0.118 lb/in³
a Lattice Constant 3.111 Å3.111 Å
c Lattice Constant 4.978 Å4.978 Å
Molecular Weight 40.989 g/mol40.989 g/mol
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 8.8 - 8.98.8 - 8.9
Band Gap 6.02 eV6.02 eV
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 180 W/m-K1250 BTU-in/hr-ft²-°F
Melting Point 2227 °C4041 °F
 
Descriptive Properties
CAS Number24304-00-5
ColorBlue WhiteHexagonal crystals
Crystal StructureHexagonalWurtzite (Zincite) Structure - Space Group P 63mc

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity
MarkeTech AN 90 Aluminum Nitride Ceramic Substrate, 98% Purity
Silicon Carbide, CVD
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride
MarkeTech AN 160 Aluminum Nitride Ceramic Substrate, 99% Purity

DSEM02 / 2919

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.