MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Pyrotek Valcor® G-AZ Pre-Cast Shapes
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Applications
  • Burner blocks
  • Skimmer blocks
  • Cover blocks
  • Specialty blocks
  • Plungers
  • Stirrers
  • Spouts
  • Feeder tubes

Advantages

  • Proven performance in molten glass contact applications
  • Smooth surface finish does not mark or streak glass
  • Molds readily available for most components

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.963 g/cc0.1070 lb/in³
Open Porosity 18 %18 %
Permeability 4.04.0ft3/hr-ft2-in/lbs/in2
 
Mechanical PropertiesMetricEnglishComments
Modulus of Rupture  0.0117 GPa
@Temperature 1538 °C
1.70 ksi
@Temperature 2800 °F
 0.0159 GPa
@Temperature 1427 °C
2.31 ksi
@Temperature 2601 °F
 0.0201 GPa
@Temperature 24.0 °C
2.92 ksi
@Temperature 75.2 °F
 0.0207 GPa
@Temperature 1260 °C
3.00 ksi
@Temperature 2300 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.10 µm/m-°C
@Temperature 20.0 °C
3.39 µin/in-°F
@Temperature 68.0 °F
Melting Point 1760 °C3200 °F
Shrinkage 0.40 %
@Temperature 1760 °C,
Time 18000 sec
0.40 %
@Temperature 3200 °F,
Time 5.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Pyrotek Valcor® G Pre-Cast Shapes
Pyrotek Wollite 30 Insulating Castable
Pyrotek F-51 Dense Machinable Board
Pyrotek O'-Sialon Non-Oxide Ceramic
CMT Materials HYTAC® LP Syntactic Plug Assist System for Heavy-Gauge Thermoforming

CPYRO155 / 1875

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.