MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol LifeSciences Tecophilic® TG-500 Hydrophilic TPU Hydrogel
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Typical Physical Test Data – Hydrogel Grade, Medical grade aliphatic, polyether-based hydrogel TPU

Features: Specially formulated to absorb large equilibrium water content. This product can absorb or transport moisture. It has been designed to dissolve in various solvents for use in solution however they can also be melt coated or extruded and can be color-matched

Process: Solution casting, coating or extrusion

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.16 g/cc1.16 g/ccASTM D792
Water Absorption 500 %500 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060Dry; ASTM D2240
Tensile Strength, Ultimate 1.72 MPa250 psiWet; ASTM D412
 6.89 MPa1000 psiDry; ASTM D412
Elongation at Break 100 %100 %Dry; ASTM D412
 200 %200 %Wet; ASTM D412

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ecoflex® C1200 F Blend Biodegradable Polyester
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene)
Goodfellow Polyacrylamide/acrylate Hydrogel
Lubrizol LifeSciences Tecophilic® TG-2000 Hydrophilic TPU Hydrogel
BASF Ecoflex® 1200 F Blend Biodegradable Polyester

PLUBR9082 / 203649

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.