System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Bhansali Engineering Abstron IM-11GM ABS Injection Molding Grade
Categories:
Polymer
;
Thermoplastic
;
ABS Polymer
Material Notes:
High Impact, High Rigidity, High Fatigue, Low Flow, Paintable
Information provided by Bhansali
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.045
g/cc
0.03775
lb/in³
ASTM D-792
Linear Mold Shrinkage
0.0040
-
0.0060
cm/cm
0.0040
-
0.0060
in/in
ASTM D-955
Melt Flow
20
g/10 min
@Load 10.0 kg,
Temperature 220 °C
20
g/10 min
@Load 22.0 lb,
Temperature 428 °F
ASTM D-1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
113
113
ASTM D-785
Tensile Strength, Yield
45.1
MPa
@Thickness 3.20 mm
6540
psi
@Thickness 0.126 in
Type 1; ASTM D-638
Flexural Yield Strength
66.7
MPa
@Thickness 6.40 mm
9670
psi
@Thickness 0.252 in
ASTM D-790
Flexural Modulus
2.26
GPa
@Thickness 6.40 mm
327
ksi
@Thickness 0.252 in
ASTM D-790
Izod Impact, Notched
2.75
J/cm
@Thickness 6.40 mm
5.14
ft-lb/in
@Thickness 0.252 in
ASTM D-256
3.4314
J/cm
@Thickness 3.20 mm
6.4284
ft-lb/in
@Thickness 0.126 in
ASTM D-256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
94.0
°C
201
°F
Method A - Annealed; ASTM D-648
Vicat Softening Point
104
°C
219
°F
Method B; ASTM D-1525
Flammability, UL94
HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
UL-94
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Bhansali Engineering Abstron IM-11B ABS Injection Molding Grade
Bhansali Engineering Abstron MIF-35 ABS Injection Molding Grade
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade
Trinseo Magnum™ 1250 BG Acrylonitrile Butadiene Styrene (ABS)
Omni Plastics OmniTech™ ABS 63 ABS
PBHANS09 / 27118
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.