MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Zirconium, Zr
Categories: Metal; Nonferrous Metal; Zirconium Alloy; Pure Element

Material Notes: This entry is for pure Zr; MatWeb also has data sheets for many Zr alloys.

Characteristics:

  • Ductile
  • Mechanical Properties similar to titanium and austenitic stainless steel
  • Excellent corrosion resistance
  • Transparent to thermal energy neutrons.
  • Forms adherent, refractory double-oxide layer above 650°C
  • Highly anisotropic, undergoes allotropic transormation from hcp-structured alpha phase to bcc-structured beta phase at 870°C

Applications:

  • Superalloys
  • Alloying with Aluminium, Copper, Magnesium or Titanium
  • Water-cooled Nuclear reactors
  • Chemical processing equipment

Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 6.53 g/cc0.236 lb/in³
Vapor Pressure  1.013e-10 bar
@Temperature 1574 °C
7.598e-8 torr
@Temperature 2865 °F
 1.013e-9 bar
@Temperature 1690 °C
7.598e-7 torr
@Temperature 3070 °F
 1.013e-8 bar
@Temperature 1822 °C
0.000007598 torr
@Temperature 3312 °F
 1.013e-7 bar
@Temperature 1976 °C
0.00007598 torr
@Temperature 3589 °F
 0.000001013 bar
@Temperature 2156 °C
0.0007598 torr
@Temperature 3913 °F
 0.00001013 bar
@Temperature 2367 °C
0.007598 torr
@Temperature 4293 °F
 0.0001013 bar
@Temperature 2620 °C
0.07598 torr
@Temperature 4750 °F
 0.001013 bar
@Temperature 2926 °C
0.7598 torr
@Temperature 5299 °F
 0.01013 bar
@Temperature 3304 °C
7.598 torr
@Temperature 5979 °F
 0.1013 bar
@Temperature 3783 °C
75.98 torr
@Temperature 6841 °F
 1.013 bar
@Temperature 4409 °C
759.8 torr
@Temperature 7968 °F
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 91.22491.2241995
Atomic Number 4040
Thermal Neutron Cross Section 0.18 barns/atom0.18 barns/atom
X-ray Absorption Edge 0.68877 Å0.68877 ÅK
 4.8938 Å4.8938 ÅLI
 5.37088 Å5.37088 ÅLII
 5.57374 Å5.57374 ÅLIII
Electronegativity 1.331.33Pauling
Ionic Radius 0.790 Å0.790 ÅCrystal Ionic Radius for Valence +4
 1.09 Å1.09 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 0.844 g/A/h0.844 g/A/h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 145145Converted from Vickers for 3000 kg load/10 mm ball. Annealed sample
Hardness, Rockwell A 4949Converted from Vickers. annealed sample
Hardness, Rockwell B 7878Converted from Vickers. Annealed sample
Hardness, Vickers 150150annealed sample
Tensile Strength, Ultimate 330 MPa47900 psiAnnealed
Tensile Strength, Yield 230 MPa33400 psiAnnealed
Elongation at Break 32 %32 %Annealed
Modulus of Elasticity 94.5 GPa13700 ksi
Poissons Ratio 0.340.34
Shear Modulus 35.3 GPa5120 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000400 ohm-cm0.0000400 ohm-cm
Magnetic Susceptibility 0.000001340.00000134cgs/g
Critical Magnetic Field Strength, Oersted 4747
Critical Superconducting Temperature 0.610 K0.610 K±0.15; 0.65, 0.95 K for omega Zr.
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 251 J/g108 BTU/lb
CTE, linear  5.80 µm/m-°C
@Temperature 20.0 - 100 °C
3.22 µin/in-°F
@Temperature 68.0 - 212 °F
 6.30 µm/m-°C
@Temperature 250 °C
3.50 µin/in-°F
@Temperature 482 °F
 6.90 µm/m-°C
@Temperature 500 °C
3.83 µin/in-°F
@Temperature 932 °F
Specific Heat Capacity 0.285 J/g-°C0.0681 BTU/lb-°F
Thermal Conductivity 16.7 W/m-K116 BTU-in/hr-ft²-°F
Melting Point 1852 °C3366 °F
Boiling Point 4377 °C7911 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.320.32650 nm; unoxidized; total
 
Processing PropertiesMetricEnglishComments
Annealing Temperature >= 705 °C>= 1300 °Fcold-rolled, in vacuum
 >= 760 °C>= 1400 °Fhot-rolled
 >= 1000 °C>= 1830 °Fsolution annealing for forged billets
 
Component Elements PropertiesMetricEnglishComments
Zirconium, Zr 100 %100 %
 
Descriptive Properties
Alpha Phase Crystal Structurehcp< 870°C
Beta Phase Crystal Structurebcc> 870°C
CAS Number7440-67-7

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium, Ti
Tungsten, W
Silicon, Si
Nickel, Ni
Zirconium Oxide, Zirconia, ZrO2

AMEZr00 / 133

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.