MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Durethan® BKV 140 H2.0 DUS008 900051 Nylon 6, Glass Fiber Reinforced, Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Filled, Impact Grade

Material Notes: PA 6, 40% glass fibers, injection molding, impact modified, heat-aging stabilized

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.46 g/cc1.46 g/ccISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 180 MPa26100 psid.a.m.; ISO 527-1, -2; 5 mm/min
Elongation at Break 3.0 %3.0 %d.a.m.; ISO 527-1, -2; 5 mm/min
Tensile Modulus 11.5 GPa1670 ksid.a.m.; ISO 527-1, -2; 1 mm/min
Flexural Strength 290 MPa
@Strain 4 %
42100 psi
@Strain 4 %
d.a.m., 2 mm/min; ISO 178-A
Flexural Modulus 10.7 GPa1550 ksid.a.m., 2 mm/min; ISO 178-A
Charpy Impact Unnotched  8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
d.a.m.; ISO 179-1eU
 8.00 J/cm²
@Temperature -30.0 °C
38.1 ft-lb/in²
@Temperature -22.0 °F
cond.; ISO 179-1eU
 8.50 J/cm²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
d.a.m.; ISO 179-1eU
 10.5 J/cm²
@Temperature 23.0 °C
50.0 ft-lb/in²
@Temperature 73.4 °F
cond.; ISO 179-1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
d.a.m.; ISO 179-1eA
 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
cond.; ISO 179-1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
d.a.m.; ISO 179-1eA
 3.00 J/cm²
@Temperature 23.0 °C
14.3 ft-lb/in²
@Temperature 73.4 °F
cond.; ISO 179-1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °F10°C/min; ISO 11357-1, -3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 290 °C500 - 554 °F
 290 °C554 °Ffor test specimens; ISO 294
Mold Temperature 80.0 °C176 °Ffor test specimens; ISO 294
 80.0 - 100 °C176 - 212 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2 - 6 hour2 - 6 hour
Moisture Content 0.030 - 0.12 %0.030 - 0.12 %residual; Karl Fischer Test
 
Descriptive Properties
ISO Short NameISO 1874-PA 6/66-HI, GHR, 14-110, GF40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Celanex® 6400-2 PBT, Mineral / Glass Reinforced
Envalior Pocan® BF 4130 XF 000000 PBT, 30% Glass Fiber
Envalior Durethan® AM 40 X H2.0 901510 Nylon 66, Glass Fiber/Mineral Reinforced
Evonik Trogamid® T-GF35 35% Glass Reinforced Amorphous Nylon
RTP Company RTP 383 Polycarbonate (PC), Carbon Fiber

PLANX0621 / 133584

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.