Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Categories:
Polymer
;
Thermoplastic
;
Liquid Crystal Polymer (LCP)
;
Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
Material Notes:
Zenite« 6130L is a lubricated 30% glass reinforced LCP resin. It is well suited for use in automotive, electrical/electronic, telecommunications, and aerospace industries.
Information provided by Celanese
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.62
g/cc
0.0585
lb/in³
ISO 1183
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
130
MPa
18900
psi
5mm/min; ISO 527-2/1A
Elongation at Break
1.8 %
1.8 %
5mm/min; ISO 527-2/1A
Tensile Modulus
13.0
GPa
1890
ksi
50mm/min; ISO 527-2/1A
Flexural Modulus
12.0
GPa
1740
ksi
ISO 178
Charpy Impact Unnotched
3.50
J/cm²
16.7
ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched
2.50
J/cm²
11.9
ft-lb/in²
ISO 179/1eA
Electrical Properties
Metric
English
Comments
Volume Resistivity
>=
1.00e+16
ohm-cm
>=
1.00e+16
ohm-cm
IEC 60093
Surface Resistance
>=
1.00e+16
ohm
>=
1.00e+16
ohm
IEC 60093
Dielectric Constant
4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
4.16
@Frequency 2.05e+9 Hz
4.16
@Frequency 2.05e+9 Hz
Dielectric Strength
36.0
kV/mm
914
kV/in
IEC 60243-1
Dissipation Factor
0.031
@Frequency 1e+6 Hz
0.031
@Frequency 1e+6 Hz
IEC 60250
0.050
@Frequency 2.05e+9 Hz
0.050
@Frequency 2.05e+9 Hz
Comparative Tracking Index
200
V
200
V
IEC 60112
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
3.00
µm/m-°C
1.67
µin/in-°F
ISO 11359-2
CTE, linear, Transverse to Flow
70.0
µm/m-°C
38.9
µin/in-°F
ISO 11359-2
Melting Point
335
°C
635
°F
10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi)
265
°C
509
°F
ISO 75-1, -2
Flammability, UL94
V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
V-0
@Thickness 0.380 mm
V-0
@Thickness 0.0150 in
Processing Properties
Metric
English
Comments
Processing Temperature
80.0
-
120
°C
176
-
248
°F
cavity
Feed Temperature
40.0
-
60.0
°C
104
-
140
°F
Zone 1
335
-
345
°C
635
-
653
°F
Zone 2
350
-
360
°C
662
-
680
°F
Zone 3
350
-
360
°C
662
-
680
°F
Zone 4
350
-
360
°C
662
-
680
°F
Die Temperature
350
-
360
°C
662
-
680
°F
Melt Temperature
350
-
360
°C
662
-
680
°F
Drying Temperature
>=
150
°C
>=
302
°F
Dry Time
3.00
hour
3.00
hour
Moisture Content
<= 0.010 %
<= 0.010 %
Injection Pressure
50.0
-
150
MPa
7250
-
21800
psi
Hold Pressure
50.0
-
150
MPa
7250
-
21800
psi
Back Pressure
<=
3.00
MPa
<=
435
psi
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
VICTREX™ PEEK 450CA30 30% Carbon Fiber Reinforced
Celanese VECTRA E130i LCP, 30% Glass Reinforced
Celanese ZENITE 6130LX LCP, 30% Glass Reinforced
Celanese Zenite® 7130 BK010 LCP (Extended Tabular Temperature Data)
Celanese Zenite® 7130 WT010 LCP (Extended Tabular Temperature Data)
PHCQ537 / 178992
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.