MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Lord Adhesives Thermoset™ TC-350 Thermally Conductive Silicone Grease
Categories: Fluid; Lubricant; Silicone Base; Silicone, Filled Grease

Material Notes: Lord TC-350 is a microelectronics-grade, silicone-based, grease compound. It offers high thermal conductivity, high temperature resistance and easy dispensability. TC-350 has been designed for use in applications with high wattage devices and where the device may later need to be easily removed. It can be used with a variety of emerging and standard devices including microprocessors, DSPs, graphic accelerators, etc. packaged in Flip Chip, PPGA, BGA, MicroBGA and other package types.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.75 g/cc2.75 g/cc
Brookfield Viscosity 50000 cP50000 cPCP52 @ 10rpm
 250000 cP250000 cPCP52 @ 1rpm
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 4.00 W/m-K27.8 BTU-in/hr-ft²-°FMathis Hot Disk Analyzer
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 5.00 °C
6.00 Month
@Temperature 41.0 °F
 
Descriptive Properties
AppearanceGray
Thixotropic Index5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NuSil G-9020 Silicone Grease
NuSil G-9000 Silicone Grease
Lord Adhesives Thermoset™ TC-330 Thermally Conductive Silicone Grease
DuPont MOLYKOTE® AS-828 Silicone Grease
NuSil G-9340 Silicone Grease

PLORD032 / 86040

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.