MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Permabond 940 Cyanoacrylate, low odor
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate adhesives on hot and humid days, is eliminated. The elimination of fogging improves the production rate of acceptable parts as well as their appearance. The adhesive is very stable and will provide optimum performance for one year when refrigerated.

Features & Benefits:

  • Low odor for improved worker comfort
  • Non-frosting –good aesthetic appearance
  • Ease of use – no mixing or heat cure
  • Bonds most materials
  • 100% reactive, no solvents.

Information provided by Permabond.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.10 g/cc1.10 g/ccUncured
Viscosity 3.0 - 10 cP
@Temperature 25.0 °C
3.0 - 10 cP
@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C35.6 - 44.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8585ISO 868
Adhesive Bond Strength 4.00 MPa580 psiPhenolic, Shear; ISO 4587
 5.00 MPa725 psiPVC, Shear; ISO 4587
 >= 5.00 MPa>= 725 psiPC, Substrate Failure, Shear; ISO 4587
 >= 6.00 MPa>= 870 psiABS, Substrate Failure, Shear; ISO 4587
 8.00 MPa1160 psiZinc, Shear; ISO 4587
 8.00 - 9.00 MPa1160 - 1310 psiAluminum, Shear; ISO 4587
 16.0 - 20.0 MPa2320 - 2900 psiSteel, Shear; ISO 4587
Impact 3.0 - 5.03.0 - 5.0kJ/m2 Adhesive Impact Strength; ASTM D950
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
Dielectric Strength 25.0 kV/mm635 kV/inDIN 53481
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°F
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 82.2 °C180 °F
Minimum Service Temperature, Air -62.2 °C-80.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 0.0333 - 0.0833 min0.000556 - 0.00139 hourNeoprene, handling time
 0.167 - 0.250 min0.00278 - 0.00417 hourSteel, handling time
 0.167 - 0.250 min0.00278 - 0.00417 hourAluminum, handling time
 0.167 - 0.250 min0.00278 - 0.00417 hourPVC, handling time
 0.167 - 0.250 min0.00278 - 0.00417 hourPhenolic resin, handling time
 0.167 - 0.250 min0.00278 - 0.00417 hourABS, handling time
 0.500 - 0.667 min0.00833 - 0.0111 hourZinc, handling time
 1440 min24.0 hourfull strength
 
Descriptive Properties
AppearanceColorlessUncured
Maximum Gap Fill (mm)0.05
Strength Retention10% at 150°CRelative to 0°C
 100% at 0°CRelative to 0°C
 30% at 100°CRelative to 0°C
 55% at -50°CRelative to 0°C
 90% at 50°CRelative to 0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Momentive Performance Materials RTV6702 One-Component,  Modified Alkoxy Adhesive Sealant, White

PPERMA50 / 56158

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.