MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis Borstar® FB1350 Medium Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Medium Density (MDPE)

Material Notes: Borstar® FB1350 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Borstar® FB1350 is well suited for mono- and coextrusion of films produced with high neck or low neck extrusion. Applications Borstar® FB1350 has been developed especially for applications like heavy-duty sack, general packaging, pouches, refuse sacks and liners, geomembranes, and blending.

Information provided by Borealis AG

Key Words: MDPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³ISO 1183
Melt Flow  0.70 g/10 min
@Load 5.00 kg,
Temperature 190 °C
0.70 g/10 min
@Load 11.0 lb,
Temperature 374 °F
ISO 1133
 15 g/10 min
@Load 21.6 kg,
Temperature 190 °C
15 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 400 %400 %ISO 527-3
Film Elongation at Break, TD 650 %650 %ISO 527-3
Tensile Modulus 0.500 GPa72.5 ksiMD; ASTM D882-A
 0.650 GPa94.3 ksiTD; ASTM D882-A
Coefficient of Friction 0.400.40ISO 8295
Elmendorf Tear Strength MD 200 g200 gISO 6383/2
Elmendorf Tear Strength TD 150 g150 gISO 6383/2
Elmendorf Tear Strength, MD 2.04 g/micron51.8 g/milISO 6383/2
Elmendorf Tear Strength, TD 26.5 g/micron673 g/milISO 6383/2
Dart Drop Test 220 g
@Thickness 0.0250 mm
0.485 lb
@Thickness 0.000984 in
ISO 7765-1
Film Tensile Strength at Break, MD 57.0 MPa8270 psiISO 527-3
Film Tensile Strength at Break, TD 48.0 MPa6960 psiISO 527-3
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 210 °C374 - 410 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® HHM TR-305 Medium density hexene copolymer
Borealis Borstar® FB2310 LLDPE for Film
Borealis Borstar® FB4370 Medium Density Polyethylene
Overview of materials for Medium Density Polyethylene (MDPE), Molded
Borealis BorSafe™ ME3445 Medium Density Polyethylene

PBOREA387 / 108646

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.