MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow INSPIRE™ 112 Performance Polymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP)

Material Notes: INSPIRE™ 112 Performance Polymer is a propylene-based resin intended for use in film and sheet extrusion.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183
Melt Flow 0.40 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.40 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6161ISO 868
Tensile Strength, Ultimate 24.0 MPa3480 psiISO 527
Film Tensile Strength at Yield, MD 29.0 MPa4210 psiISO 527-3
Film Tensile Strength at Yield, TD 24.0 MPa3480 psiISO 527-3
Tensile Strength, Yield 28.0 MPa4060 psiISO 527
Film Elongation at Break, MD 600 %600 %ISO 527-3
Film Elongation at Break, TD 710 %710 %ISO 527-3
Elongation at Break 25 %25 %ISO 527
Elongation at Yield 14 %14 %ISO 527
Tensile Modulus 1.15 GPa167 ksiISO 527
Flexural Modulus 1.35 GPa196 ksiISO 527
Secant Modulus, MD 1.10 GPa160 ksi1% Secant; ISO 527-3
Secant Modulus, TD 0.950 GPa138 ksi1% Secant; ISO 527-3
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -20.0 °C
5.71 ft-lb/in²
@Temperature -4.00 °F
ISO 180
 23.0 kJ/m²
@Temperature -10.0 °C
10.9 ft-lb/in²
@Temperature 14.0 °F
ISO 180
 46.0 kJ/m²
@Temperature 23.0 °C
21.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Dart Drop Test 170 g0.375 lbMethod A; ISO 7765-1
Film Tensile Strength at Break, MD 52.0 MPa7540 psiISO 527-3
Film Tensile Strength at Break, TD 39.0 MPa5660 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 164 °C327 °FDow Method (DSC)
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °FISO 75B
Vicat Softening Point 148 °C298 °FISO 306A
Shrinkage 1.5 %1.5 %ISO 2577

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow C133-02 Polypropylene Impact Copolymer Resin
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes
Total PPC 1645 Polypropylene, Heterophasic Copolymer, Pipes
Dow CYCLOTENE™ 3022-57 Bisbenzocyclobutene (BCB) Electronic Resin
Dow ELITE™ 5100G Enhanced Polyethylene Resin

PDOW1136 / 30340

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.