MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 12, Carbon Fiber Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Carbon Fiber Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.04 - 1.50 g/cc0.0376 - 0.0542 lb/in³Average value: 1.16 g/cc Grade Count:57
Filler Content 10.0 - 59.0 %10.0 - 59.0 %Average value: 37.9 % Grade Count:8
Water Absorption 0.200 - 1.50 %0.200 - 1.50 %Average value: 0.712 % Grade Count:13
Moisture Absorption at Equilibrium 0.0700 - 0.700 %0.0700 - 0.700 %Average value: 0.446 % Grade Count:7
Water Absorption at Saturation 1.10 %1.10 %Average value: 1.10 % Grade Count:6
Additive Loading 15.0 - 30.0 %15.0 - 30.0 %Average value: 25.0 % Grade Count:5
Particle Size 35.0 - 100 µm35.0 - 100 µmAverage value: 58.8 µm Grade Count:3
Linear Mold Shrinkage 0.000 - 0.00600 cm/cm0.000 - 0.00600 in/inAverage value: 0.00245 cm/cm Grade Count:31
Linear Mold Shrinkage, Transverse 0.00100 - 0.00550 cm/cm0.00100 - 0.00550 in/inAverage value: 0.00311 cm/cm Grade Count:22
Melt Flow 3.14 - 50.0 g/10 min3.14 - 50.0 g/10 minAverage value: 16.6 g/10 min Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 77.0 - 96.077.0 - 96.0Average value: 84.0 Grade Count:3
Ball Indentation Hardness 100 - 135 MPa14500 - 19600 psiAverage value: 120 MPa Grade Count:5
Tensile Strength, Ultimate 25.0 - 1750 MPa3630 - 254000 psiAverage value: 186 MPa Grade Count:49
Tensile Strength, Yield 28.8 - 103 MPa4180 - 15000 psiAverage value: 63.9 MPa Grade Count:3
Elongation at Break 1.00 - 14.3 %1.00 - 14.3 %Average value: 3.61 % Grade Count:49
Modulus of Elasticity 2.20 - 100 GPa319 - 14500 ksiAverage value: 15.8 GPa Grade Count:50
Flexural Yield Strength 58.1 - 900 MPa8430 - 131000 psiAverage value: 228 MPa Grade Count:32
Flexural Modulus 1.83 - 95.0 GPa265 - 13800 ksiAverage value: 15.3 GPa Grade Count:35
Flexural Strain at Break 2.30 - 5.40 %2.30 - 5.40 %Average value: 3.38 % Grade Count:9
Izod Impact, Notched 0.214 - 2.67 J/cm0.401 - 5.00 ft-lb/inAverage value: 0.979 J/cm Grade Count:15
Izod Impact, Unnotched 0.850 - 10.7 J/cm1.59 - 20.0 ft-lb/inAverage value: 5.05 J/cm Grade Count:14
Izod Impact, Notched (ISO) 9.00 - 28.0 kJ/m²4.28 - 13.3 ft-lb/in²Average value: 16.6 kJ/m² Grade Count:13
 5.00 - 18.0 kJ/m²
@Temperature -30.0 - -30.0 °C
2.38 - 8.57 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 12.5 kJ/m² Grade Count:13
Izod Impact, Unnotched (ISO) 45.0 - 87.0 kJ/m²21.4 - 41.4 ft-lb/in²Average value: 61.0 kJ/m² Grade Count:14
 41.0 - 90.0 kJ/m²
@Temperature -30.0 - -30.0 °C
19.5 - 42.8 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 61.5 kJ/m² Grade Count:14
Charpy Impact Unnotched 0.550 - 8.30 J/cm²2.62 - 39.5 ft-lb/in²Average value: 5.27 J/cm² Grade Count:15
 3.99 - 7.90 J/cm²
@Temperature -30.0 - -30.0 °C
19.0 - 37.6 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 5.49 J/cm² Grade Count:8
Charpy Impact, Notched 0.210 - 2.80 J/cm²0.999 - 13.3 ft-lb/in²Average value: 1.39 J/cm² Grade Count:17
 0.500 - 1.60 J/cm²
@Temperature -30.0 - -30.0 °C
2.38 - 7.61 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 0.840 J/cm² Grade Count:8
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00500 - 7.80e+14 ohm-cm0.00500 - 7.80e+14 ohm-cmAverage value: 2.69e+13 ohm-cm Grade Count:30
Surface Resistance 50.0 - 2.90e+14 ohm50.0 - 2.90e+14 ohmAverage value: 1.12e+13 ohm Grade Count:27
 
Thermal PropertiesMetricEnglishComments
CTE, linear 3.00 - 48.6 µm/m-°C1.67 - 27.0 µin/in-°FAverage value: 18.8 µm/m-°C Grade Count:7
 25.0 - 27.0 µm/m-°C
@Temperature 40.0 - 100 °C
13.9 - 15.0 µin/in-°F
@Temperature 104 - 212 °F
Average value: 26.0 µm/m-°C Grade Count:1
CTE, linear, Transverse to Flow 3.00 - 150 µm/m-°C1.67 - 83.3 µin/in-°FAverage value: 94.6 µm/m-°C Grade Count:7
 150 - 300 µm/m-°C
@Temperature 40.0 - 100 °C
83.3 - 167 µin/in-°F
@Temperature 104 - 212 °F
Average value: 225 µm/m-°C Grade Count:1
Melting Point 176 - 184 °C349 - 363 °FAverage value: 178 °C Grade Count:21
Maximum Service Temperature, Air 80.0 - 150 °C176 - 302 °FAverage value: 125 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 170 - 179 °C338 - 354 °FAverage value: 174 °C Grade Count:8
Deflection Temperature at 1.8 MPa (264 psi) 140 - 200 °C284 - 392 °FAverage value: 167 °C Grade Count:28
Deflection Temperature at 8.0 MPa 85.0 - 175 °C185 - 347 °FAverage value: 133 °C Grade Count:18
Vicat Softening Point 160 - 210 °C320 - 410 °FAverage value: 181 °C Grade Count:12
Glass Transition Temp, Tg 37.0 - 41.0 °C98.6 - 106 °FAverage value: 39.3 °C Grade Count:3
Flammability, UL94 HBHBGrade Count:21
 
Processing PropertiesMetricEnglishComments
Melt Temperature 200 - 300 °C392 - 572 °FAverage value: 257 °C Grade Count:35
Mold Temperature 40.0 - 120 °C104 - 248 °FAverage value: 84.8 °C Grade Count:33
Drying Temperature 79.4 - 100 °C175 - 212 °FAverage value: 85.9 °C Grade Count:28
Moisture Content 0.0570 - 0.150 %0.0570 - 0.150 %Average value: 0.113 % Grade Count:12
Dew Point -40.0 °C-40.0 °FAverage value: -40.0 °C Grade Count:7
Injection Pressure 30.0 - 103 MPa4350 - 15000 psiAverage value: 79.6 MPa Grade Count:11

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 12, 30% Glass Fiber Filled
Overview of materials for Nylon 12
Overview of materials for Nylon 12, 20% Glass Fiber Filled
Overview of materials for Nylon 12, 40% Glass Fiber Filled
Overview of materials for Nylon 12, Graphite Filled

O2649 / 78071

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.