MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lanxess Addonyl® TT Nylon Casting Aid
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Cast Nylon 6, a plastic of high molecular weight, is produced through an anionic polymerization of caprolactam. During the pressureless casting process the monomeric caprolactam melt is poured into the mold and directly polymerized by a specific chemical reaction and then forms a semi-finished product or molding. Addonyl® TT is an isocyanate crosslinker with a pyrogenous silicic acid (< 1%) as a fluxing agent. The additive is used as an activator during the production of cast nylon (PA-6 G). In combination with the catalyst Addonyl® Kat NL and other products from the Addonyl series users can combine various properties to tailor materials specifically to requirements.

Addonyl® TT is used as an activator in cast nylon (PA-6 G) in order to extend the pouring time.

Use: The reactivity of the polymerizing melt is influenced by various factors. Lanxess recommends an activator concentration of at least 0.5% by weight. The quantity of the activator to be used, however, decisively depends on the size and form of the casting mold.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³
 
Thermal PropertiesMetricEnglishComments
Melting Point >= 140 °C>= 284 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 100 °C212 °F
Mold Temperature 160 °C320 °F
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Appearancewhite to light-yellowish powder
Content24 percentNCO
 98 percentAddonyl TT

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Master Bond MB600S Aqueous Based Sodium Silicate System for EMI/RFI Shielding
Aluminum Phosphate, AlPO4
Sodium Aluminate, NaAlO2
MV Labs AL900 AlPO4 Aluminum phosphate
Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating

PLANY8222 / 208615

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.