MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ecomass® 1050CO94 Copper Filled Polyamide
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Nontoxic alternative to Lead (Pb), weighting and balancing applications
  • Moderate Specific Gravity
  • Copper Powder Filled Polyamide (PA) Alloy
  • Good Toughness

Information provided by Technical Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 6.00 g/cc6.00 g/ccASTM D792
Linear Mold Shrinkage 0.0060 - 0.0090 cm/cm0.0060 - 0.0090 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 31.0 MPa4500 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Tensile Modulus 9.10 GPa1320 ksiASTM D638
Flexural Strength 46.9 MPa6800 psiASTM D790
Flexural Modulus 5.29 GPa767 ksiASTM D790
Izod Impact, Notched 0.587 J/cm1.10 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C250 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 204 - 254 °C400 - 490 °F
Mold Temperature 57.2 - 82.2 °C135 - 180 °F
Drying Temperature 73.9 °C165 °F
Dry Time 4 hour4 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL B63 CU90 Nylon 6.6 for injection molding, 90% copper filled
Ecomass® 1007TU78 Tungsten Filled COPA
Celanese Nilit FRIANYL A63 CU90 Nylon 6.6 for injection molding, 90% copper filled
Ecomass® 1007ZC85 Stainless Steel Filled COPA
Overview of materials for Aluminum Alloy

PECOM30 / 35440

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.