MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company PermaStat® 601 FR Acrylonitrile Butadiene Styrene (ABS), Glass Fiber - Flame Retardant - ESD Protection - Permanently Anti-static
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Glass Fiber Filled, Flame Retardant

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.34 g/cc1.34 g/ccASTM D 792
Filler Content 10 %10 %Primary Additive
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
@Thickness 3.17 mm
0.0020 - 0.0040 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 41.4 MPa6000 psiASTM D 638
Elongation at Break 3.0 - 5.0 %3.0 - 5.0 %ASTM D 638
Tensile Modulus 3.10 GPa450 ksiASTM D 638
Flexural Strength 75.8 MPa11000 psiASTM D 790
Flexural Modulus 3.10 GPa450 ksiASTM D 790
Izod Impact, Notched 0.427 J/cm
@Thickness 3.17 mm
0.800 ft-lb/in
@Thickness 0.125 in
D 256
Izod Impact, Unnotched 2.67 J/cm
@Thickness 3.17 mm
5.00 ft-lb/in
@Thickness 0.125 in
ASTM D4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+9 - 9.90e+10 ohm-cm1.00e+9 - 9.90e+10 ohm-cmASTM D 257
Surface Resistance 1.00e+9 - 9.90e+10 ohm1.00e+9 - 9.90e+10 ohmESD STM11.11
Surface Resistivity per Square 1.00e+10 - 9.90e+11 ohm1.00e+10 - 9.90e+11 ohmASTM D 257
Static Decay <= 2.0 sec<= 2.0 secMIL-PRF-81705D, 5kV to 50 V, 12% RH; FTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0
@Thickness 1.59 mm
V-0
@Thickness 0.0625 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 238 °C390 - 460 °F
Mold Temperature 48.9 - 93.3 °C120 - 200 °F
Drying Temperature 82.2 °C180 °F
Dry Time 2 hour2 hour
Moisture Content 0.10 %0.10 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow HDPE 25455N High Density Polyethylene
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
Celanese Celcon® M90-45XAP® POM, Specialty

PQZWA2612 / 91262

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.