MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating
Categories: Polymer; Film; Thermoplastic; Poly (P-Xylylene)

Material Notes: Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 450°C) and those in which long-term UV stability is required. Parylene HT also has a low coefficient of friction and dielectric constant, and a high penetrating ability.

SCS Parylene conformal coatings are ultra-thin, pinhole-free polymer coatings that provide a number of high-value surface treatment properties such as excellent moisture, chemical and dielectric barrier properties, thermal and UV stability, and dry-film lubricity. Parylene coatings are used in a number of applications throughout the medical device, electronics, automotive, military and aerospace industries.

Information provided by Specialty Coating Systems (SCS) .

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Permeability 0.220 g mil/ (m2 day)
@Temperature 38.0 °C
0.0142 g mil/ (100 in2 day)
@Temperature 100 °F
100% RH; ASTM F1249
Density 1.32 g/cc0.0477 lb/in³ASTM D1505
Water Absorption <= 0.010 %
@Time 86400 sec
<= 0.010 %
@Time 24.0 hour
ASTM D570
Oxygen Transmission 23.5 cc-mm/m²-24hr-atm
@Temperature 25.0 °C
59.7 cc-mil/100 in²-24hr-atm
@Temperature 77.0 °F
ASTM D1434
Nitrogen Transmission 4.80 cc-mm/m²-24hr-atm
@Temperature 25.0 °C
12.2 cc-mil/100 in²-24hr-atm
@Temperature 77.0 °F
ASTM D1434
Carbon Dioxide Transmission 95.4 cc-mm/m²-24hr-atm
@Temperature 25.0 °C
242 cc-mil/100 in²-24hr-atm
@Temperature 77.0 °F
ASTM D1434
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 122122ASTM D785
Tensile Strength 51.7 MPa7500 psi
Tensile Strength, Yield 34.5 MPa5000 psiASTM D882
Elongation at Break <= 200 %<= 200 %ASTM D882
Elongation at Yield 2.0 %2.0 %ASTM D882
Modulus of Elasticity 2.55 GPa370 ksiSecant; ASTM D5026
Coefficient of Friction, Dynamic 0.130.13ASTM D1894
Coefficient of Friction, Static 0.150.15ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+17 ohm-cm2.00e+17 ohm-cm50% RH; ASTM D257
Surface Resistance 5.00e+15 ohm5.00e+15 ohm50% RH; ASTM D257
Dielectric Constant  2.17
@Frequency 1e+6 Hz
2.17
@Frequency 1e+6 Hz
ASTM D150
 2.2
@Frequency 1000 Hz
2.2
@Frequency 1000 Hz
ASTM D150
 2.21
@Frequency 60 Hz
2.21
@Frequency 60 Hz
ASTM D150
Dielectric Strength 213 kV/mm5400 kV/inASTM D149
Dissipation Factor  <= 0.00020
@Frequency 60 Hz
<= 0.00020
@Frequency 60 Hz
ASTM D150
 0.0010
@Frequency 1e+6 Hz
0.0010
@Frequency 1e+6 Hz
ASTM D150
 0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 36.0 µm/m-°C20.0 µin/in-°Fvia TMA
Specific Heat Capacity 1.04 J/g-°C0.249 BTU/lb-°F
Thermal Conductivity 0.0960 W/m-K0.666 BTU-in/hr-ft²-°FASTM 1461
Melting Point >= 500 °C>= 932 °Fvia DSC
Maximum Service Temperature, Air 350 °C662 °FContinuous; ASTM 5026
 450 °C842 °FShort Term; ASTM 5026
Softening Point 377 °C711 °FT5 Point; modulus = 690 MPa (100,000 psi)
 >= 450 °C>= 842 °FT4 point; modulus = 70 MPa (10,000 psi)
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.559
@Wavelength 589.3 nm
1.559
@Wavelength 589.3 nm
nD; ASTM D542
Transmission, Visible 88 %
@Wavelength 400 nm
88 %
@Wavelength 400 nm
UV Transmittance  <= 1.0 %
@Wavelength 273 nm
<= 1.0 %
@Wavelength 273 nm
cutoff
 80 %
@Wavelength 300 nm
80 %
@Wavelength 300 nm
 88 %
@Wavelength 350 nm
88 %
@Wavelength 350 nm
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
BiocompatibilityISO 10993

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parylene Coating Services C Poly (P-Xylylene)
Parylene Coating Services N Poly (P-Xylylene)
Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating
Specialty Coating Systems Parylene N Poly (P-Xylylene) Coating
Parylene Coating Services D Poly (P-Xylylene)

PPARYL93 / 171629

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.