MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Geon® Performance Solutions Vinyl Rigid Molding M4825 Polyvinyl Chloride, Rigid
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Rigid Grade

Material Notes: ** NOTE: UL REGULATORY LISTING PENDING

Geon Performance Solutions was created from PolyOne in 2019.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inASTM D955
Spiral Flow 109.22 cm43.000 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8484ASTM D2240
Tensile Strength, Yield 62.7 MPa9090 psiType I, 51 mm/min; ASTM D638
Elongation at Break 16 %16 %Type I, 51 mm/min; ASTM D638
Tensile Modulus 3.29 GPa477 ksiType I, 51 mm/min; ASTM D638
Flexural Strength 96.5 MPa14000 psiASTM D790
Flexural Modulus 3.24 GPa470 ksiASTM D790
Izod Impact, Notched 0.530 J/cm
@Thickness 3.18 mm,
Temperature 23.0 °C
0.993 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi)  63.9 °C
@Thickness 6.35 mm
147 °F
@Thickness 0.250 in
Annealed; ASTM D648
 66.1 °C
@Thickness 6.35 mm
151 °F
@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  60.0 °C
@Thickness 6.35 mm
140 °F
@Thickness 0.250 in
Annealed; ASTM D648
 63.0 °C
@Thickness 6.35 mm
145 °F
@Thickness 0.250 in
Unannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 4.0 %
@Thickness 3.81 mm
4.0 %
@Thickness 0.150 in
ASTM D1003
Transmission, Visible 75 %
@Thickness 3.81 mm
75 %
@Thickness 0.150 in
ASTM D1003
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 204 °C390 - 399 °F
 
Descriptive Properties
AppearanceClear/Transparent
FeaturesGeneral Purpose
 High Flow
FormsPellets
Generic MaterialPVC, Rigid
Generic NamePolyvinyl Chloride, Rigid (PVC, Rigid)
Product Description** NOTE: UL REGULATORY LISTING PENDING
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesGeneral Purpose

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Geon® Performance Solutions Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid
Geon® Performance Solutions Vinyl Rigid Molding M5240 Natural Polyvinyl Chloride, Rigid
Bayshore Vinyl Compounds BRC R409002 Molding Compound
Stratasys® RGD4825-DM Simulated Polypropylene Digital Material
Avient Novablend™ 6602 Polyvinyl Chloride, Rigid

PH0POL0567 / 145136

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.