MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCoat 8709-12/AboCure 50-12 Silver-Filled Electrically Conductive Epoxy Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: AboCoat 8709-12/AboCure 50-12 is a versatile silver-epoxy high-solids coating with good conductive and adhesive properties. It is successful as a conductive compound for most electronic uses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 87.5 %87.5 %
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.010 ohm<= 0.010 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 110 °C230 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 - 180 min
@Temperature 50.0 - 100 °C
0.500 - 3.00 hour
@Temperature 122 - 212 °F
Optional
 >= 1440 min
@Temperature 22.0 - 30.0 °C
>= 24.0 hour
@Temperature 71.6 - 86.0 °F
Pot Life 60 min60 min
 
Descriptive Properties
ColorGray
Metal (%)80.6of vehicle
Parts by Weight (pbw)100AboCoat 8709-12
 2.5AboCure 50-12
ViscosityMedium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Epoxy, Electrically Conductive
Epoxy Technology EPO-TEK® E2101 Electrically Conductive, Silver Epoxy
Aptek DIS-A-PASTE 2310-PMF Thermally conductive adhesive/encapsulant
Abatron AboCoat 8401-1 A/B Silver-Filled Electrically Conductive Epoxy Compound
Master Bond EP51AN Thermally Conductive Adhesive System

PABC847 / 107831

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.