MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Novec™ 71DA Engineered Fluid
Categories: Fluid

Material Notes: 3M™ Novec™ 71DA Engineered Fluid is a hydrofluoroether, Methyl Nonafluorobutyl Ether (C4F9OCH3), in an azeotrope formulation with trans-1,2-dichloroethylene (t-DCE) and ethanol. This mixture is a true azeotrope, with constant vapor and liquid composition at its boiling point. Novec 71DA fluid is ideal for defluxing and degreasing tasks and is intended to replace ozone-depleting materials in many applications as well as certain aqueous cleaning processes and solvent coating applications. This Novec product has zero ozone depletion potential and other favorable environmental properties (see Table 2). Novec 71DA fluid has a recommended time-weighted average exposure guideline of 750 ppm for the 3M™ Novec™ 7100 Engineered Fluid component (eight hour average), 200 ppm for trans-1,2-dichloroethylene (t-DCE) and 1000 ppm for ethyl alcohol. These exposure guidelines suggest there is a large margin of safety for use of Novec 71DA fluid in its intended cleaning applications. The increased solvency and low surface tension, nonflammability and constant composition during boiling of Novec 71DA fluid make it ideal for immersion defluxing and degreasing applications. The ethanol component of Novec 71DA fluid provides enhanced removal of ionic contaminants.

Applications:

  • Cleaning, rinsing and drying agent; coating solvent
    • Cleaning of oils, greases, waxes, handling oils and solder flux residue
    • Precision coating of silicones and other lubricants

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³Liquid
Viscosity 0.45 cP0.45 cP
Vapor Pressure 0.508 bar381 torr
Surface Tension 16.4 dynes/cm16.4 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 209.3 J/g90.06 BTU/lb
Boiling Point 40.0 °C104 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Novec™ 7000 Engineered Fluid
3M Novec™ 7100DL Engineered Fluid
3M Novec™ 7100 Engineered Fluid
3M Novec™ 649 Engineered Fluid
3M Novec™ 774 Engineered Fluid

PMM33105 / 167852

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.